Mechanical Properties Metric English Comments
Modulus of Elasticity 0.0700 GPa
10.2 ksi
ISO 527-2
Total EVA 1003 VN 4 Ethylene Vinyl Acetate Copolymer - Blown Film
EVA 1003 VN 4 is made by a high pressure tubular process. Grade for flexible films with very high transparency and outstanding mechanical properties. Contains an antioxidant.Application examples: ..
Modulus of Elasticity 0.0700 GPa
10.2 ksi
ISO 527-2
Total EVA 1005 VN 35 Ethylene Vinyl Acetate Copolymer - Blown Film
EVA 1005 VN 35 is made by a high pressure tubular process. Grade for flexible films, with high transparency and outstanding mechanical properties. Contains NO antioxidant.Information provided by T..
Modulus of Elasticity 0.0700 GPa
10.2 ksi
ISO 527
Lucobit Lucobit® 1235 Ethylene Copolymer Bitumen
Lucobit® combines the positive properties of polyolefins and bitumen. The material is black and consists of mixtures based on high quality polyethylene copolymers with varying additions of special..