Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.0500 - 1.40 GPa @Temperature 50.0 - 100 °C |
7.25 - 203 ksi @Temperature 122 - 212 °F |
Average value: 0.422 GPa Grade Count:5 |
Overview of materials for Polyvinylidinefluoride (PVDF), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyvinylidinefluoride (PVDF), Molded/Extruded". Each property range of values reported is minimum and m.. |
|||
Modulus of Elasticity | 0.0500 GPa | 7.25 ksi | ASTM D638 |
Micropol E188 Rotational molding powder based on a random EVA copolymer Information provided by Micropol Limited |
|||
Modulus of Elasticity | 0.0500 GPa | 7.25 ksi | |
Lehmann & Voss LUVOCOM® 100-7846 Thermoplastic polyurethane, with aramid reinforcement Applications: Improved friction and wear behaviour. Emergency running property.dynamic stressBearings, sleeves, sliding elements, chair rollers, handles.Information provided by Lehmann & Voss & Co.K.. |
|||
Modulus of Elasticity | 0.0500 GPa | 7.25 ksi | |
DuPont Elvax® 460 Ethylene-Vinyl Acetate Copolymer Resin Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with.. |
|||
Modulus of Elasticity | 0.0500 GPa | 7.25 ksi | ISO 527-2 |
Total EVA 1020 VN 5 Ethylene Vinyl Acetate Copolymer - Blown Film EVA 1020 VN 5 is made by a high pressure tubular process. Grade for very flexible films with very high transparency and good mechanical properties. Contains an antioxidant.Application examples: Ch.. |
|||
Modulus of Elasticity | 0.0500 GPa | 7.25 ksi | ASTM D638 |
Arkema Group Pebax® 4033 Polyether Block Amide (PEBA) Typical application: Mechanical partsInformation provided by Arkema Group |
|||
Modulus of Elasticity | 0.0500 - 3.07 GPa | 7.25 - 445 ksi | Average value: 0.460 GPa Grade Count:35 |
Overview of materials for Polyether Ester Elastomer This property data is a summary of similar materials in the MatWeb database for the category "Polyether Ester Elastomer". Each property range of values reported is minimum and maximum values of appr.. |