Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Creep Modulus, 1 hour | 9800 - 19600 MPa | 1.42e+6 - 2.84e+6 psi | Average value: 14000 MPa Grade Count:6 |
Overview of materials for Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled". Specific grades with glass content between 25% an.. |
|||
Tensile Creep Modulus, 1 hour | 9800 MPa | 1.42e+6 psi | ISO 899-1 |
Lanxess Pocan® B 3235 901510 PBT, 30% Glass Fiber PBT, 30% glass fibers, injection molding |
|||
Tensile Creep Modulus, 1 hour | 9800 MPa | 1.42e+6 psi | ISO 899-1 |
Lanxess Pocan® B 3235 000000 PBT, 30% Glass Fiber PBT, 30% glass fibers, injection molding |