Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Creep Modulus, 1 hour | 2500 MPa @Time 3600 sec |
363000 psi @Time 1.00 hour |
ISO 899-1 |
DuPont Performance Polymers Crastin® FG6130 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)< Unreinforced High Viscosity Polybutylene Terephthalate Developed for Food Contact Applications and Extrusion and Injection Molding Crastin FG6130 NC010 is an unreinforced medium high viscosity polyb.. |
|||
Tensile Creep Modulus, 1 hour | 2500 MPa @Time 3600 sec |
363000 psi @Time 1.00 hour |
ISO 899-1 |
DuPont Performance Polymers Crastin® S650FR NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)< Unreinforced Flame Retardant Polybutylene Terephthalate Crastin S650FR is an unreinforced flame retardant polybutylene terephthalate for injection molding.Information provided by DuPont Performance .. |
|||
Tensile Creep Modulus, 1 hour | 2500 MPa | 363000 psi | |
Ineos ABS NOVODUR® P3T ABS, Injection Grade
(discontinued **) Injection molding grade, higher heat resistance.Applications: Automotive industry.Information provided by the manufacturer.Novodur is produced by Styrolution (2014). This grade was discontinued pri.. |