Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Creep Modulus, 1 hour | 1000 - 3400 MPa | 145000 - 493000 psi | Average value: 2320 MPa Grade Count:14 |
Overview of materials for Nylon 66, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Tensile Creep Modulus, 1 hour | 1000 MPa | 145000 psi | ISO 899-1 |
Lanxess Durethan® A 30 H2.0 901510 Nylon 66 PA 66 standard injection molding grade, non-reinforced, very easy release, good heat-ageing resistanceApplication Examples: terminal blocks, cable clips, bobbins, gearwheels |
|||
Tensile Creep Modulus, 1 hour | 1000 MPa | 145000 psi | ISO 899-1 |
Lanxess Durethan® A 30 000000 Nylon 66 PA 66, standard injection molding grade, non-reinforced, very easy release, normal solidificationApplication Examples: terminal blocks, cable clips, bobbins, gearwheels |
|||
Tensile Creep Modulus, 1 hour | >= 1000 MPa | >= 145000 psi | ASTM D638 |
Centro Plastica CiPiTENE® Recycled High Density Polyethylene Granules Bottle Grade. Source: Italian post-consumer plastic bottles coming from collection of municipal waste and selected by PE/PP matrix. |