Mechanical Properties Metric English Comments
Tensile Creep Modulus, 1 hour 1000 - 3400 MPa
145000 - 493000 psi
Average value: 2320 MPa Grade Count:14
Overview of materials for Nylon 66, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced". Each property range of values reported is minimum and maximum values of appropr..
Tensile Creep Modulus, 1 hour 1000 MPa
145000 psi
ISO 899-1
Lanxess Durethan® A 30 H2.0 901510 Nylon 66
PA 66 standard injection molding grade, non-reinforced, very easy release, good heat-ageing resistanceApplication Examples: terminal blocks, cable clips, bobbins, gearwheels
Tensile Creep Modulus, 1 hour 1000 MPa
145000 psi
ISO 899-1
Lanxess Durethan® A 30 000000 Nylon 66
PA 66, standard injection molding grade, non-reinforced, very easy release, normal solidificationApplication Examples: terminal blocks, cable clips, bobbins, gearwheels
Tensile Creep Modulus, 1 hour >= 1000 MPa
>= 145000 psi
ASTM D638
Centro Plastica CiPiTENE® Recycled High Density Polyethylene Granules
Bottle Grade. Source: Italian post-consumer plastic bottles coming from collection of municipal waste and selected by PE/PP matrix.