Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Creep Modulus, 1 hour | 7100 MPa | 1.03e+6 psi | |
BASF Luranyl® KR 2403 G6 Polyphenylene Ether + Styrene-Butadiene Blend, 30% Glass Fiber Reinforced General-purpose grade with 30% glass fiber for parts requiring especially good resistance to heat deformation.Applications: parts for hot-water contact, pump housings, fan blades.Data was collected .. |