Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact Strength | 755 kJ/m² | 359 ft-lb/in² | At 23°C; ASTM D1822 |
DuPont Elvax® 260 Ethylene-Vinyl Acetate Copolymer Resin Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with.. |
|||
Tensile Impact Strength | 755 kJ/m² | 359 ft-lb/in² | At 23°C; ASTM D1822S |
DuPont Nucrel® 925 Ethylene-Methacrylic Acid Copolymer Resin Nucrel® 925 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for .. |