Polymer Property : Tensile Impact Strength = 358 kJ/m²
Polymer Property :
Tensile Impact Strength =
358 kJ/m²
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Tensile Impact Strength
358
kJ/m²
170
ft-lb/in²
ASTM D1822
Global POM-100 High Viscosity Acetal Homopolymer
Information provided by Global Polymers Corporation.