Polymer Property : Tensile Impact Strength = 262 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Impact Strength 550 kJ/m²
262 ft-lb/in²
23°C; ASTM D-1822
ExxonMobil Iotek® 7010 Zinc Ionomer Molding/Extrusion Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A zinc ionomer with excellent flexibility, abrasion resistance, impact strength and tensile strength. This ionomer has outstanding adhesion to glas..
Tensile Impact Strength 550 kJ/m²
262 ft-lb/in²
23°C; ASTM D-1822
ExxonMobil Iotek® 8020 Sodium Ionomer Molding/Extrusion Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A sodium ionomer with excellent abrasion resistance, impact strength, hardness and tensile strength. IOTEK ionomers provide superb low temperature ..