Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact Strength | 218 kJ/m² | 104 ft-lb/in² | notched, 23°C; ISO 8256/1 |
DSM Arnitel® EM402-L Polyether Ester Elastomer (European Grade)
(discontinued **) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Impact Strength | 218 kJ/m² | 104 ft-lb/in² | 23°C; ISO 8256/1 |
DSM Arnitel® EM400 40 Shore D, Injection or Extrusion Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Impact Strength | 218 kJ/m² | 104 ft-lb/in² | notched, 23°C; ISO 8256/1 |
DSM Arnitel® EM400 Polyether Ester Elastomer (European and Asian Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Impact Strength | 218 kJ/m² | 104 ft-lb/in² | 23°C; ISO 8256/1 |
DSM Arnitel® EM402-L Injection Molding; Coating Grade Copolyester Elastomer (North America)
(discontinued **) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |