Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact Strength | 21.0 kJ/m² | 10.0 ft-lb/in² | |
ITW Devcon 10 minuteâ„¢ Epoxy, Black Information provided by ITW Devcon |
|||
Tensile Impact Strength | 21.0 kJ/m² | 10.0 ft-lb/in² | |
ITW Devcon 10 minuteâ„¢ Epoxy, Clear Information provided by ITW Devcon |
|||
Tensile Impact Strength | 21.0 kJ/m² | 10.0 ft-lb/in² | |
ITW Devcon Epoxy Plusâ„¢ 25 Grey Information provided by ITW Devcon |