Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact Strength | 120 kJ/m² | 57.1 ft-lb/in² | S bar; ASTM D 1822 |
Chevron Phillips HiD® 9404 HDPE Blow Molding Resin
(discontinued **) Resin Type: linear copolymerCharacteristics: medium molecular weight distributions, wide range of processing conditions, low parison sag, good stress crack resistance. Federal specification LP390C .. |
|||
Tensile Impact Strength | 120 kJ/m² | 57.1 ft-lb/in² | |
LyondellBasell Lupolen® 5621 D HDPE Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Tensile Impact Strength | 120 kJ/m² | 57.1 ft-lb/in² | |
LyondellBasell Lupolen® 6021 D HDPE, Blow Molding Grade Easy flow, blow molding grade for small, rigid, thin-walled containers (up to 5 l), pots (up to 1 l), bottles and canisters (up to 5 l) for packaging mineral oil, antifreeze, brake fluid; drink bott.. |
|||
Tensile Impact Strength | 120 kJ/m² | 57.0 ft-lb/in² | ASTM D-1822 |
Axiall 9175 White 10 Rigid PVC, Molding, White 10 Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Impact Strength | 120 kJ/m² | 57.1 ft-lb/in² | Notched, -30°C; ISO 8256 |
Total Finathene® 53080 HDPE, blow molding, sheet
(discontinued **) Finathene E® 53080 is a high density polyethylene produced by the slurry loop low pressure polymerization process. Finathene E® 53080 has been especially developed for the production of containers.. |