Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.02099 GPa | 3.045 ksi | |
Spartech E65490 General Purpose PVC First choice for compounds meeting the stringent requirements of Spiral Hose, Automotive, Housewares, Farm Equipment, Coated Fencing and numerous other applications including Lawn & Garden Wheels. B.. |
|||
100% Modulus | 0.02099 GPa | 3.045 ksi | Plasticizer conc. in vinyl film 33 phr; ASTM D638 |
BASF Palamoll® 656 Polymeric Plasticizer Description: Palamoll® 656 is a high viscosity polymeric plasticizer that is compatible with PVC. It is based on adipic acid and polyhydric alcohols. It is resistant to oils, fats, aliphatic hydro.. |