Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.0113 GPa | 1.64 ksi | ASTM D412 |
Mearthane Durethaneâ„¢ S DS-555D Solid Polyurethane Elastomer TDI backbone: ether.Summary: Durethane S is a solid urethane elastomer. Formulations are individually compounded and tested to meet OEM requirements for durometer, tensile strength, tear strength, .. |
|||
100% Modulus | 0.0113 GPa | 1.64 ksi | JIS-K-6723 |
Denka VINYKON W5120 PVC, W grade for non-migratory sheath and special items A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |
|||
100% Modulus | 0.0113 GPa | 1.64 ksi | ASTM D1414, ASTM D412 |
DuPont Performance Polymers Kalrez® AeroSeal™ 7800 Fluoroelastomer Kalrez AeroSeal™ 7800* perfluoroelastomer parts are a specialty black product that meets the requirements of Aerospace Material Specification (AMS) 7257. It offers outstanding thermal stability and.. |
|||
100% Modulus | 0.0113 GPa | 1.64 ksi | ASTM D-638 |
Axiall 38951 Wire & Cable Flexible PVC Low cost AWM jacket for SPT, SVT, SJT applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |