Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : 100% Modulus = 1.35 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
100% Modulus 0.00931 GPa
1.35 ksi
ASTM D412
S&E Specialty Polymers GA-2190E-FR CLEAR PVC
Application: Specialty clear, 60° C insulating compound designed for excellent clarity and sunlight resistance.Information provided by S&E Specialty Polymers
100% Modulus 0.00931 GPa
1.35 ksi
ASTM D412
S&E Specialty Polymers TufTech™ GA-7056-1002 PVC Compound
Application: A 75°C Jacketing Compound UL approved for 720 hr. sunlight resistance. Suitable for use in direct burial applications.Information provided by S&E Specialty Polymers
100% Modulus 0.00930 GPa
1.35 ksi
ASTM D412
Precision Polymer Engineering Perlast® G70H Perfluoroelastomer
Special, pure white compound with high temperature properties and wide chemical resistance. Has excellent chemical resistance, steam resistance and mechanical properties. Extremely low outgassing p..
100% Modulus 0.00931 GPa
1.35 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 120 PHR N339 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00931 GPa
1.35 ksi
Spartech E65080 General Purpose PVC
First choice for compounds meeting the stringent requirements of Spiral Hose, Automotive, Housewares, Farm Equipment, Coated Fencing and numerous other applications including Lawn & Garden Wheels. B..
100% Modulus 0.00931 GPa
1.35 ksi
ASTM D412
Teknor Apex UNIPRENE® 7100-40D Thermoplastic Elastomer
Information provided by Teknor Apex Company
100% Modulus 0.00931 GPa
1.35 ksi
500 mm/min; ASTM D 412
Zylog Neoplast® 180 HOFR Thermoplastic Vulcanizate
Neoplast 180 HOFR is a flame retardant thermoplastic vulcanizate (TPV) compound, based on polyolefin chemistry, suitable for Injection Molding and Extrusion applications.RoHS Compliant, UV Stabilize..
100% Modulus 0.00931 GPa
1.35 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 120 PHR N339 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00931 GPa
1.35 ksi
ASTM D-638
Axiall 8852 Moldings & Extrusions Flexible PVC
General purpose compound recommended for extrusion applications. Contains a biocide and is UV stabilized.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
100% Modulus 0.00931 GPa
1.35 ksi
ASTM D-638
Axiall EX1188B Wire & Cable Flexible PVC
UL 360 jacket compound. 105°C air; 60°C oil.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
100% Modulus 0.00930 GPa
1.35 ksi
Die C; Cross direction; ASTM D412
Teknor Apex Sarlink® 4139D Thermoplastic Elastomer
A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4139D is a high hardness grade possessing exceptional tensile strength, superior compression set, chemical re..
100% Modulus 0.00930 GPa
1.35 ksi
Die C; Cross direction; ASTM D412
Teknor Apex Sarlink® 4439D Thermoplastic Elastomer
A NSF certified, highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4439D is a high hardness grade possessing exceptional tensile strength, superior compression s..
Copyright © lookpolymers.com All Rights Reserved