Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00827 GPa | 1.20 ksi | ASTM D412 |
S&E Specialty Polymers TufTech™ GA-3099LF PVC Compound Application: RoHS compliant, 80°C AWM insulation and jacketing compoundInformation provided by S&E Specialty Polymers |
|||
100% Modulus | 0.00830 GPa | 1.20 ksi | |
Taiwan PU Corporation TPUI-E90 General Grade, Injection Molding Polyester Base TPU Thermoplastic Polyurethane (TPU), General Grade, Polyester Base, Injection MoldingInformation provided by Taiwan PU Corporation. |
|||
100% Modulus | 0.00830 GPa | 1.20 ksi | |
Taiwan PU Corporation TPUI-H90 High Hydrolysis Resistance, Injection Molding Polyether Base TPU Thermoplastic Polyurethane (TPU), High Hydrolysis Resistance, Polyether Base, Injection MoldingInformation provided by Taiwan PU Corporation. |
|||
100% Modulus | 0.00830 GPa | 1.20 ksi | |
Taiwan PU Corporation TPUI-L85 Low Temperature Resistance, Injection Molding Polyester Base TPU Thermoplastic Polyurethane (TPU), Low Temperature Resistance, Polyester Base, Injection MoldingInformation provided by Taiwan PU Corporation. |
|||
100% Modulus | 0.00827 GPa | 1.20 ksi | |
Colorite Polymers 7812 Clear Injection Molding Vinyl Compound Description: Clear non-toxic vinyl compounds are utilized by the health and medical industries for injection molding of various components such as drip chambers, connectors, valves, etc. The vinyl c.. |
|||
100% Modulus | 0.00827 GPa | 1.20 ksi | ASTM D638 |
Colorite Polymers 93-732A General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
100% Modulus | 0.00827 GPa | 1.20 ksi | |
Colorite Polymers Self Frosting™ 7811SF Vinyl Compound Description: Colorite has developed a family of vinyl compounds to satisfy the needs of those who need a smooth, low gloss, low friction surface for the products that they produce. Historically, thi.. |
|||
100% Modulus | 0.00827 GPa | 1.20 ksi | ASTM D-638 |
Axiall 68141 Wire & Cable Flexible PVC 90°C rated, non-lead stabilized compound designed for use as an SE and USE jacket.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.00827 GPa | 1.20 ksi | ASTM D-638 |
Axiall 8840 Moldings & Extrusions Flexible PVC Economical general purpose extrusion compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.00827 GPa | 1.20 ksi | ASTM D-638 |
Axiall 12802 Wire & Cable Flexible PVC Non-lead stabilized general purpose jacket recommended for 75C applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.00827 GPa | 1.20 ksi | ASTM D-638 |
Axiall 12860 Wire & Cable Flexible PVC 80C liquid tight conduit.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.00827 GPa | 1.20 ksi | ASTM D-638 |
Axiall 14840 Wire & Cable Flexible PVC General purpose jacketing compound recommended for a maximum service temperature of 80°C.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.00827 GPa | 1.20 ksi | ASTM D-638 |
Axiall 12862 Wire & Cable Flexible PVC Non-lead 80C liquid tight conduit compound according to UL360.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.00827 GPa | 1.20 ksi | ASTM D638 |
Colorite Polymers 7900FR General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
100% Modulus | 0.00827 GPa | 1.20 ksi | ASTM D-638 |
Axiall 19801 Wire & Cable Flexible PVC Primary insulation and jacketing compound recommended for 105°C applications at a minimum wall of 15 mils. CSA approved AWM, SVT, SJT, ST, SVTO, SVTOO, SJTO, SJTOO, STO, STOO constructions. 60°C.. |
|||
100% Modulus | 0.00827 GPa | 1.20 ksi | ASTM D-638 |
Axiall 38901 Wire & Cable Flexible PVC Non-lead flame retardant flexible PVC compound suitable for integral conduit jackets.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.00827 GPa | 1.20 ksi | |
Colorite Polymers 7811 Clear Extrusion Vinyl Compound Description: Clear non-toxic vinyl compounds are utilized by the health and medical industries for the extrusion of various components for the production of devices. The vinyl components used in pre.. |
|||
100% Modulus | 0.00827 GPa | 1.20 ksi | ASTM D412 |
DuPont Performance Polymers Kalrez® 1045 Fluoroelastomer DuPont™ Kalrez® 1045 perfluoroelastomer parts are a specialty white product that is reinforced with a mineral filler that is highly resistant to oxidizing environments (carbon black-filled product.. |
|||
100% Modulus | 0.00827 GPa | 1.20 ksi | ASTM D-638 |
Axiall 14811 Wire & Cable Flexible PVC Matte finish general purpose jacket compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |