Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00800 GPa | 1.16 ksi | ASTM D412 |
Precision Polymer Engineering Perlast® G60H Perfluoroelastomer Special, pure white compound with excellent high temperature properties and wide chemical resistance. Extremely low outgassing properties.Applications: For use in applications which require exposur.. |
|||
100% Modulus | >= 0.00800 GPa | >= 1.16 ksi | DIN 53504 |
NEXA® PFX8014 Perfluoroelastomer NEXA produces sealing elements for extreme and critical applications, particularly where high temperature, wet conditions (steam/water), purity and chemical resistance are important factors to consi.. |
|||
100% Modulus | >= 0.00800 GPa | >= 1.16 ksi | DIN 53504 |
NEXA® PFX8034 Perfluoroelastomer NEXA produces sealing elements for extreme and critical applications, particularly where high temperature, wet conditions (steam/water), purity and chemical resistance are important factors to consi.. |
|||
100% Modulus | 0.00800 GPa | 1.16 ksi | ASTM D412 |
Lubrizol Advanced Materials PEARLTHANE® D16N90UV Thermoplastic Polyurethane Elastomer
(discontinued **) PEARLTHANE® D16N90UV is a polyether-based TPU, containing an anti-UV additive, supplied in form of transparent, colorless pellets, offering adequate hardness, excellent mechanical properties and go.. |
|||
100% Modulus | 0.00800 GPa | 1.16 ksi | ISO 37 |
Huntsman AVALON® 90 AB Thermoplastic Polyurethane Performance Features: AVALON® injection molding products are trusted worldwide to deliver:Outstanding flex performanceExcellent slip resistancePerfect surface definitionTransparency and transluce.. |
|||
100% Modulus | 0.00800 GPa | 1.16 ksi | ASTM D412 |
Lubrizol Advanced Materials PEARLTHANE® 11T92EM Thermoplastic Polyurethane Elastomer PEARLTHANE® 11T92EM is a polyester based TPU, supplied in form of translucent, colourless or slightly yellowish pellets, combining hardness with excellent mechanical properties. It can be extrude.. |
|||
100% Modulus | 0.00800 GPa | 1.16 ksi | ISO 37 |
Huntsman AVALON® 90 ABR Thermoplastic Polyurethane Introduction: AVALON 90 ABR is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 90 ABR is part of the AVALON Performance Range and offers a premium soling .. |
|||
100% Modulus | 0.00800 GPa | 1.16 ksi | ISO 37 |
Huntsman AVALON® 90 AK Thermoplastic Polyurethane Introduction: AVALON 90 AK is a part of the AVALON Crystal Range and offers a specially designed, flexible material wit a higher degree of transparency compared with conventional TPU at the same har.. |
|||
100% Modulus | 0.00800 GPa | 1.16 ksi | ISO 37 |
Huntsman AVALON® 90 AKU Thermoplastic Polyurethane Introduction: AVALON 90 AKU is a part of the AVALON Crystal Range and offers a specially designed, flexible material wit a higher degree of transparency compared with conventional TPU at the same ha.. |
|||
100% Modulus | 0.00800 GPa | 1.16 ksi | DIN 53504 |
Huntsman IROGRAN® A 92 E 4738 Polyester-Based TPU-Injection Extrusion Grade Introduction: IROGRAN A 92 E 4738 is a white-colored, thermoplastic special-polyester-polyurethane for injection molding applications. Additional characteristics of the product are flexibility and h.. |
|||
100% Modulus | 0.00800 GPa | 1.16 ksi | ASTM D412 |
Lubrizol STAT-RITE® S-1100 Static Dissipative TPU Description: Stat-Rite® S1100 is a static dissipative TPU alloy. Stat-Rite S-1100 utilizes the patented Stat-Rite inherently dissipative polymer (IDP) alloy system to provide clean, permanent ESD p.. |
|||
100% Modulus | 0.00800 GPa | 1.16 ksi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-2190 Polycaprolactone Based TPU Low compression set, good oil resistance & hydrolytic stability, good abrasion resistance, low temperature flexibilityInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
100% Modulus | 0.00800 GPa | 1.16 ksi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-7185 Polycaprolactone Based TPU Higher mechanical strength, good hydrolytic stability & chemical resistance, weather resistance, heat & fungus resistanceInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
100% Modulus | 0.00800 GPa | 1.16 ksi | DIN 53504 |
Lubrizol ESTANE® 58447 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
100% Modulus | 0.00800 GPa | 1.16 ksi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-1290 Polyester Based TPU Good mechanical properties, good extrusion stability, low costInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
100% Modulus | 0.00800 GPa | 1.16 ksi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-1590 Polyester Based TPU Low cost, good mechanical properties, good processabilityInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
100% Modulus | 0.00800 GPa | 1.16 ksi | ASTM D412 |
Dow PELLETHANE® 2101-85A Polyurethane Elastomer (Ether-Ether Hybrid)
(discontinued **) Description: PELLETHANE® 2101-85A offers good low temperature properties, fast cycle time, and good hydrolytic stability. Applications include: seals, gaskets, animal tags, molding applications, ho.. |