Mechanical Properties Metric English Comments
100% Modulus 0.005886 GPa
0.8537 ksi
JIS-K-6723
Denka LCS Z1075 Thermoplastic Elastomer, Extrusion grade (general)
"DENKA LCS" combines low hardness with a rubber-like texture, having a low permanent compressive distortion/permanent elongation, and is a thermoplastic elastomer that closely resembles vulcanized r..
100% Modulus 0.005886 GPa
0.8537 ksi
JIS-K-6723
Denka REOMER G G3010 Thermoplastic Elastomer, For Extrusion
Essentially a thermoplastic elastomer with the characteristics of PVC resin and rubber, with excellent rubber-like elasticity. Offers excellent rubbery characteristics, such as permanent compressive..
100% Modulus 0.005886 GPa
0.8537 ksi
JIS-K-6723
Denka REOMER G G5369 Thermoplastic Elastomer, For Extrusion
Essentially a thermoplastic elastomer with the characteristics of PVC resin and rubber, with excellent rubber-like elasticity. Offers excellent rubbery characteristics, such as permanent compressive..
100% Modulus 0.005886 GPa
0.8537 ksi
JIS-K-6723
Denka VINYKON G5369 PVC, W grade for non-migratory sheath and special items
A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding..
100% Modulus 0.005886 GPa
0.8537 ksi
JIS-A-5756
Denka VINYKON S3095K PVC, S grade for refrigerator gaskets
A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding..