Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00520 GPa | 0.754 ksi | ASTM D412-80 |
DuPont Performance Polymers Hypalon® 40 Chlorosulfonated Polyethylene Rubber, Carbon Black Filled Compound
(d Carbon black compound with 100 parts Hypalon; 27.8 parts sublimed litharge dispersion; 55 parts carbon black; 55 parts aromatic process oil; 0.5 parts MTBS; and 2 parts Tetrone® A rubber accelerato.. |
|||
100% Modulus | 0.00520 GPa | 0.754 ksi | ASTM D412-80 |
DuPont Performance Polymers Hypalon® 48 Chlorosulfonated Polyethylene Rubber, Uncured Carbon Black Filled Compound
& Carbon black compound with 100 parts Hypalon; 100 parts carbon black; 4 parts magnesia; and 1.5 parts propylene glycol. Physical property data below (except mooney viscosity) are for uncured film. .. |
|||
100% Modulus | 0.00520 GPa | 0.754 ksi | TPE-0153 (ASTM D 412) |
Advanced Elastomer Systems Trefsin® 3101-85 W305 Thermoplastic Rubber
(discontinued **) A black thermoplastic elastomer with excellent permeation resistance to water, air and other gases. It can be processed using injection molding, extrusion, blow molding or other melt processing tec.. |
|||
100% Modulus | 0.00520 GPa | 0.754 ksi | TPE-0153 (ASTM D 412) |
Advanced Elastomer Systems Trefsin® 3201-85 W305 Thermoplastic Rubber
(discontinued **) A natural thermoplastic elastomer with excellent permeation resistance to water, air and other gases. It can be processed using injection molding, extrusion, blow molding or other melt processing t.. |
|||
100% Modulus | 0.00520 GPa | 0.754 ksi | DIN 53504 |
Huntsman IROGRAN® A 78 P 4766 TPU-Polyether Excellent resistance to hydrolysis and microbial attack. Suggested for injection molding and extrusion.Information provided by Huntsman |
|||
100% Modulus | 0.00520 GPa | 0.754 ksi | DIN 53504 |
Huntsman IROGRAN® A 86 E 4486 Polyester-Based TPU-Injection Extrusion Grade Introduction: IROGRAN A 86 E 4486 is a thermoplastic polyester- polyurethane for injection molding and extrusion applications. Additional characteristics of the product are excellent mechanical prop.. |
|||
100% Modulus | 0.00520 GPa | 0.754 ksi | ASTM D412 |
Lubrizol STAT-RITE® E-1150 Ether-Type Static Dissipative Polymer Description: IStat-Rite® E-1150 blend is a static dissipative thermoplastic polyurethane (TPU) alloy. Stat-Rite E-1150 utilizes the patented Stat-Rite inherently dissipative polymer (IDP) alloy sys.. |
|||
100% Modulus | 0.00520 GPa | 0.754 ksi | ASTM D412 |
Lubrizol ESTANE® 58630 Ether Based Thermoplastic Polyurethane Features: Good physical properties, hydrolysis resistance, low temperature performance and abrasion along with wide processing window for extrusion and low surface tack.Uses: Blown and flat die/cast.. |
|||
100% Modulus | 0.00520 GPa | 0.754 ksi | ASTM D412 |
Lubrizol Estane® 2103-80PF Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Film and profile resinAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in.. |
|||
100% Modulus | 0.00520 GPa | 0.754 ksi | |
Lubrizol ESTANE® 5701 Ester Based Thermoplastic Polyurethane Features: Displays Low Temperature Flexibility and Abrasion Resistance.Uses: Audio Tape Binder and Screen Printing Inks, Inks and Lacquers, Cast Film for LaminationAvailable in Americas and AsiaInfo.. |
|||
100% Modulus | 0.00520 GPa | 0.754 ksi | ASTM D638 |
ELASTO UK Dryflex® 650900 TPE, Improved Compression Set and High Temperature Resistance, 90A Hardness The VTC TPE Group have developed endless formulations to fulfill different properties and application requirements to optimize the finished component. This grade is designed with improved compressi.. |
|||
100% Modulus | 0.00520 GPa | 0.754 ksi | ASTM D412 |
C.O.I.M. LARIPUR® LPR8025 Special Adipate Ester Polyurethane Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |
|||
100% Modulus | 0.00520 GPa | 0.754 ksi | ISO 37 |
AlphaGary Evoprene™ G 927 SEBS Thermoplastic Elastomer Evoprene™ G compounds are styrene – ethylene butylene –styrene base thermoplastic elastomer with related hydrogenated block copolymers. These polymers are fully saturated so the resistance to oxi.. |