Polymer Property : 100% Modulus = 0.750 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
100% Modulus 0.00517 GPa
0.750 ksi
ASTM D412
Teknor Apex UNIPRENE® 7100-80 Thermoplastic Elastomer
Information provided by Teknor Apex Company
100% Modulus 0.00517 GPa
0.750 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 60 PHR N330 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00517 GPa
0.750 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 90 PHR N774 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00517 GPa
0.750 ksi
ASTM D412
Elastocon TPE Technologies Elastocon® 8078N Thermoplastic Elastomer
Elastocon® 8078N is a colorable thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8078N is FDA compliant and well suited..
100% Modulus 0.00517 GPa
0.750 ksi
ASTM D412
DuPont Performance Polymers Kalrez® Spectrum™ 0040 Fluoroelastomer
Kalrez® Spectrum™ 0040 perfluoroelastomer parts are specifically designed for low-temperature environments where significant chemical resistance is required. Proprietary polymer and cure technolog..
100% Modulus 0.00517 GPa
0.750 ksi
Colorite Polymers Flexchem 6051-02 Vinyl Compound
Description: The Flexchem "51" series is a group of translucent, flexible, non-toxic vinyl compounds which were specifically developed to replace silicone in various applications. These compounds ut..
100% Modulus 0.00517 GPa
0.750 ksi
ASTM D-638
Axiall 8700 Moldings & Extrusions Flexible PVC
General purpose, matte-finish extrusion compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
100% Modulus 0.00517 GPa
0.750 ksi
Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C
3M Dyneon™ FT 2320 Fluoroelastomer
3M™ Dyneon™ Fluoroelastomer FT 2320 can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formul..
100% Modulus 0.00517 GPa
0.750 ksi
ASTM D-638
Axiall 1601 Clear 7002 Flexible PVC
Flexible polyvinyl chloride compound formulated for USP Class VI applications. The compound possesses exceptional clarity.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation ..
100% Modulus 0.00517 GPa
0.750 ksi
ASTM D-638
Axiall 18753 Wire & Cable Flexible PVC
Non-lead stabilized, fungus resistant 105 C rated jacket compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
100% Modulus 0.00517 GPa
0.750 ksi
ASTM D-638
Axiall 6652 Moldings & Extrusions Flexible PVC
General purpose clear molding and extrusion compound with good processing characteristics and good low temperature properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporati..
100% Modulus 0.00517 GPa
0.750 ksi
ASTM D-638
Axiall 8730 Moldings & Extrusions Flexible PVC
A high quality, profile extrusion compound recommended for those applications where exceptional low temperature performance is required.Information provided by Georgia GulfGeorgia Gulf became Axiall..
100% Modulus 0.00517 GPa
0.750 ksi
ASTM D-638
Axiall 8747 Moldings & Extrusions Flexible PVC
Economical general purpose molding and extrusion compound with good flex whitening resistance especially in darker colors.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation i..
100% Modulus 0.00517 GPa
0.750 ksi
ASTM D-638
Axiall 10701 Wire & Cable Flexible PVC
General purpose 80°C compound with good low temperature properties recommended for 15 mil wall and larger.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
100% Modulus 0.00517 GPa
0.750 ksi
ASTM D638
Colorite Polymers 6575 General Purpose Vinyl Compound
Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r..
100% Modulus 0.00517 GPa
0.750 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 60 PHR N330 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00517 GPa
0.750 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 90 PHR N774 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..