Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | >= 0.00500 GPa | >= 0.725 ksi | DIN 53504 |
NEXA® PFX8050 Perfluoroelastomer NEXA produces sealing elements for extreme and critical applications, particularly where high temperature, wet conditions (steam/water), purity and chemical resistance are important factors to consi.. |
|||
100% Modulus | 0.00500 GPa | 0.725 ksi | ASTM D412 |
Lubrizol Advanced Materials PEARLTHANE® 16N80 Thermoplastic Polyurethane Elastomer
(discontinued **) PEARLTHANE® 16N80 is a polyether-based TPU, supplied in form of translucent, colourless or slightly yellowish pellets, combining hardness with excellent mechanical properties and excellent hydrolys.. |
|||
100% Modulus | 0.00500 GPa | 0.725 ksi | Injection molded parts; DIN 53504 |
Huntsman IROGRAN® A 85 E 4607 E TPU-Polyester Introduction: IROGRAN A 85 E 4607 is a thermoplastic polyether- polyurethane intended for extrusion and injection molding applications. Additional characteristics of the product are excellent mechan.. |
|||
100% Modulus | 0.00500 GPa | 0.725 ksi | ISO 527-2/5A/500 |
Lubrizol Advanced Materials PEARLTHANE® 11T80 Thermoplastic Polyurethane Elastomer Type : Pearlthane® 11T80 is a polycaprolactone copolyester-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Combining hardness with excellent mechanical pr.. |
|||
100% Modulus | 0.00500 GPa | 0.725 ksi | ASTM D412 |
Lubrizol Advanced Materials PEARLTHANE® 12F75UV Thermoplastic Polyurethane Elastomer PEARLTHANE® D12F75UV is a UV resistant standard polyester based TPU supplied in form of translucent, colorless or slightly yellowish pellets, featuring a low melting point and very low gel conten.. |
|||
100% Modulus | 0.00500 GPa | 0.725 ksi | ISO 37 |
Huntsman AVALON® 80 AE Thermoplastic Polyurethane Performance Features: AVALON® injection molding products are trusted worldwide to deliver:Outstanding flex performanceExcellent slip resistancePerfect surface definitionTransparency and transluce.. |
|||
100% Modulus | 0.00500 GPa | 0.725 ksi | ISO 37 |
Huntsman AVALON® 80 AHT DP Thermoplastic Polyurethane Performance Features: AVALON® injection molding products are trusted worldwide to deliver:Outstanding flex performanceExcellent slip resistancePerfect surface definitionTransparency and transluce.. |
|||
100% Modulus | 0.00500 GPa | 0.725 ksi | ASTM D412 |
Lubrizol Advanced Materials PEARLTHANE® Clear 15N80 Thermoplastic Polyurethane Elastomer PEARLTHANE® CLEAR 15N80 is a polyether copolymer-based TPU, supplied in form of translucent, colorless, combining low hardness with excellent mechanical properties and excellent hydrolysis resist.. |
|||
100% Modulus | 0.00500 GPa | 0.725 ksi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-1180 Polyester Based TPU Excellent mechanical properties, high abrasion resistance, tear resistance, short cycle timeInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
100% Modulus | 0.00500 GPa | 0.725 ksi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-A885 Aliphatic TPU Non-yellowish, high tensile strength, good abrasion resistance, excellent hydrolytic stability, fungus resistance, low temperature flexibilityInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
100% Modulus | 0.00500 GPa | 0.725 ksi | ISO 37 |
Lubrizol ESTANE® GP80AB Ester Based Thermoplastic Polyurethane Type: Estane® GP 80AB is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b.. |
|||
100% Modulus | 0.00500 GPa | 0.725 ksi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-1680AB Polyester Based TPU Stable melt viscosity, outstanding toughness & tear resistance, good workability for high frequency weldingInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
100% Modulus | 0.00500 GPa | 0.725 ksi | ASTM D638 |
ELASTO UK Dryflex® 500850S SEBS Based Material, Unfilled Qualities, 85A Hardness, Translucent The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
100% Modulus | 0.00500 GPa | 0.725 ksi | ASTM D638 |
ELASTO UK Dryflex® 600850S SEBS Based Material, Filled Qualities, 85A Hardness, Natural The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
100% Modulus | 0.00500 GPa | 0.725 ksi | ASTM D638 |
ELASTO UK Dryflex® 600900S SEBS Based Material, Filled Qualities, 90A Hardness, Natural The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
100% Modulus | 0.00500 GPa | 0.725 ksi | ASTM D638 |
ELASTO UK Dryflex® 602850S SEBS Based Material, Filled Qualities, 85A Hardness, Black The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
100% Modulus | 0.00500 GPa | 0.725 ksi | ASTM D638 |
ELASTO UK Dryflex® 602900S SEBS Based Material, Filled Qualities, 90A Hardness, Black The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
100% Modulus | 0.00500 GPa | 0.725 ksi | ASTM D 638 |
API Megol AM DP2395/85 SEBS Adhesion Modified Overmolding for Polar Polymers Over-molding allows for the creation of composite finished products in a single phase, removing the need for successive gluing or mechanical fixing steps. This also reduces environmental impact as .. |
|||
100% Modulus | 0.00500 GPa | 0.725 ksi | ASTM D-638 |
Axiall 8710 Moldings & Extrusions Flexible PVC Low gravity extrusion compound with excellent low temperature properties. Designed for use in weatherstrips and flexible gaskets. Excellent for co-extrusion with rigid PVC.Information provided by .. |
|||
100% Modulus | 0.00500 GPa | 0.725 ksi | ASTM D-638 |
Axiall 8740 Moldings & Extrusions Flexible PVC General purpose extrusion compound recommended for use in weatherstrips, screen spline, extruded shapes and flexible gaskets.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporatio.. |
|||
100% Modulus | 0.00500 GPa | 0.725 ksi | ASTM D-638 |
Axiall 8743 Moldings & Extrusions Flexible PVC A high quality extrusion compound recommended for weatherstrips, extruded shapes and flexible gaskets.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.00500 GPa | 0.725 ksi | ASTM D638 |
Colorite Polymers 6588 Non-Phthalate 88 Series Vinyl Compound Description: The Colorite 88 series is a family of vinyl non-toxic compounds formulated to provide excellent low temperature flexibility characteristics. These compounds are designed for outside doo.. |
|||
100% Modulus | 0.00500 GPa | 0.725 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 90 PHR Hi-Sil 233 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00500 GPa | 0.725 ksi | DIN 53504 |
Lubrizol ESTANE® 58206 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
100% Modulus | 0.00500 GPa | 0.725 ksi | Cured 7 min at 177°C and Post Cured 2 hr at 232°C |
DuPont Performance Polymers VTR 8525 (GBLT-S) GLT 505 Formulation
(discontinued **) FormulationViton® GLT 505 |