Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.0044145 GPa | 0.64028 ksi | JIS-K-6723 |
Denka LCS Z1070 Thermoplastic Elastomer, Extrusion grade (general) "DENKA LCS" combines low hardness with a rubber-like texture, having a low permanent compressive distortion/permanent elongation, and is a thermoplastic elastomer that closely resembles vulcanized r.. |
|||
100% Modulus | 0.0044145 GPa | 0.64028 ksi | JIS-A-5756 |
Denka VINYKON S3029A PVC, S grade for window frame gaskets A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |