Mechanical Properties Metric English Comments
100% Modulus 0.00328 GPa
0.475 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR N220 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00328 GPa
0.475 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR N220 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00328 GPa
0.475 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 45 PHR Mistron Vapor Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00328 GPa
0.475 ksi
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 0.5 PHR Sulfur
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
100% Modulus 0.00328 GPa
0.475 ksi
ASTM D-638
Axiall 8630 Moldings & Extrusions Flexible PVC
Extrusion compound recommended for extruded shapes and other applications where a matte finish is desired.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
100% Modulus 0.00328 GPa
0.475 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 45 PHR Mistron Vapor Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00328 GPa
0.475 ksi
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 0.5 PHR Sulfur
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
100% Modulus 0.00328 GPa
0.475 ksi
ASTM D638
Colorite Polymers 5790 General Purpose Vinyl Compound