Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00317 GPa | 0.460 ksi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, Hardness 70A MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
100% Modulus | 0.00317 GPa | 0.460 ksi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, Hardness 70A MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
100% Modulus | 0.00317 GPa | 0.460 ksi | ASTM D638 |
Colorite Polymers 5543 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
100% Modulus | 0.00317 GPa | 0.460 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 3.0 PHR MBTS Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
100% Modulus | 0.00317 GPa | 0.460 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 3.0 PHR MBTS Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |