Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.002943 GPa | 0.4269 ksi | JIS-K-6723 |
Denka REOMER G G3000 Thermoplastic Elastomer, For Extrusion Essentially a thermoplastic elastomer with the characteristics of PVC resin and rubber, with excellent rubber-like elasticity. Offers excellent rubbery characteristics, such as permanent compressive.. |
|||
100% Modulus | 0.002943 GPa | 0.4269 ksi | JIS-K-6723 |
Denka REOMER G G8250 Thermoplastic Elastomer, For Injection Molding Essentially a thermoplastic elastomer with the characteristics of PVC resin and rubber, with excellent rubber-like elasticity. Offers excellent rubbery characteristics, such as permanent compressive.. |