Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00130 GPa | 0.189 ksi | |
Kuraray HYBRAR® H7125 Hydrogenated Thermoplastic Rubber Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubb.. |
|||
100% Modulus | 0.00130 GPa | 0.189 ksi | |
Kuraray SEPTON® H5125 Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubb.. |
|||
100% Modulus | 0.00130 GPa | 0.189 ksi | Die C; Flow direction; ASTM D412 |
Teknor Apex Sarlink® 3135 Thermoplastic Elastomer A low hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3135 can be processed by injection molding or extrusion for ap.. |
|||
100% Modulus | 0.00130 GPa | 0.189 ksi | Die C; Flow direction; ASTM D412 |
Teknor Apex Sarlink® 3440 Thermoplastic Elastomer A NSF certified, low hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inject.. |
|||
100% Modulus | 0.00130 GPa | 0.189 ksi | Die C; Cross direction; ASTM D412 |
Teknor Apex Sarlink® 4145 Thermoplastic Elastomer A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4145 is a low hardness grade possessing exceptional tensile strength, superior compression set, chemical re.. |
|||
100% Modulus | 0.00130 GPa | 0.189 ksi | Die C; Cross direction; ASTM D412 |
Teknor Apex Sarlink® 4445 Thermoplastic Elastomer A NSF certified, highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4445 is a low hardness grade possessing exceptional tensile strength, superior compression s.. |
|||
100% Modulus | 0.00130 GPa | 0.189 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 2.0 PHR Di-Cup 40C MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00130 GPa | 0.189 ksi | ISO 37 |
ELASTO UK Dryflex® 5029-104 TPE, Modified Injection Molding Grade for Door Stops The VTC TPE Group have developed endless formulations to fulfill different properties and application requirements to optimize the finished component. VTC Dryflex® 5029-104 is specifically designe.. |
|||
100% Modulus | 0.00130 GPa | 0.189 ksi | ISO 37 |
ELASTO UK Dryflex® 8014-101 Flame Retardant TPE for Extrusion, Black Vitaprene® thermoplastic elastomers combine the performance of most vulcanized rubber with the process properties of thermoplastics. Vitaprene® compounds permit sophisticated component design and.. |
|||
100% Modulus | 0.00130 GPa | 0.189 ksi | ISO 37 |
ELASTO UK Dryflex® 8014-101 Flame Retardant TPE for Injection Molding, Black Dryflex® thermoplastic elastomers combine the performance of most vulcanized rubber with the process properties of thermoplastics. Dryflex® compounds permit sophisticated component design and thu.. |
|||
100% Modulus | 0.00130 GPa | 0.189 ksi | ASTM D638 |
ELASTO UK Mediprene™ 500520M TPE, Medical Applications, 52A Hardness All Mediprene™ compounds are designed and manufactured for use in medical and pharmaceutical applications. In both medical and food contact areas, high application demands are found, such as:Low e.. |
|||
100% Modulus | 0.00130 GPa | 0.189 ksi | ASTM D412 |
3M 551 Polyurethane Adhesive Sealant 3M™ 500-Series Polyurethane Construction Sealant, Polyurethane Sealant and Polyurethane Adhesive Sealant products are one component, moisture curing products which form permanent elastic bonds. The.. |
|||
100% Modulus | 0.00130 GPa | 0.189 ksi | Die C; Flow direction; ASTM D412 |
Teknor Apex Sarlink® 3140 Thermoplastic Elastomer A low hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3140 can be processed by injection molding or extrusion for appl.. |
|||
100% Modulus | 0.00130 GPa | 0.189 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 2.0 PHR Di-Cup 40C MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00130 GPa | 0.189 ksi | ISO/R527 |
Polykemi AB POLYelast TPE ZS606 Thermoplastic Elastomer, SEBS/SBS-based Information provided by Polykemi AB |