Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.0234 GPa | 3.40 ksi | ASTM D412 |
SK Chemicals SKYTHANE® S155D Polyester Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
100% Modulus | 0.0234 GPa | 3.40 ksi | ASTM D412 |
Lubrizol Estane® ALR E68D-V Thermoplastic Polyurethane Type: Estane® ALR E68D-V is a clear aliphatic thermoplastic polyurethane (TPU).Features: Non-yellowing with good mechanical properties.Available in AmericasInformation Provided by The Lubrizol Corp.. |
|||
100% Modulus | 0.0234 GPa | 3.40 ksi | ASTM D-638 |
Axiall 8621 Moldings & Extrusions Flexible PVC High quality, semi-rigid extrusion compound especially formulated for extruded T-moldings and other shapes where uniform flow through the die is required.Information provided by Georgia GulfGeorgia .. |