Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.0145 GPa | 2.10 ksi | ASTM D412 |
S&E Specialty Polymers G-4285UV PVC Application: UV resistant, PVC material designed for profile extrusion applications.Information provided by S&E Specialty Polymers |
|||
100% Modulus | 0.0145 GPa | 2.10 ksi | |
Spartech 2885-92 General Purpose PVC First choice for compounds meeting the stringent requirements of Spiral Hose, Automotive, Housewares, Farm Equipment, Coated Fencing and numerous other applications including Lawn & Garden Wheels. B.. |
|||
100% Modulus | 0.0145 GPa | 2.11 ksi | |
Spartech E65390 General Purpose PVC First choice for compounds meeting the stringent requirements of Spiral Hose, Automotive, Housewares, Farm Equipment, Coated Fencing and numerous other applications including Lawn & Garden Wheels. B.. |
|||
100% Modulus | 0.0145 GPa | 2.10 ksi | ASTM D412 |
Teknor Apex Uniprene® 50D Polyvinyl Chloride, Flexible Features: High Elastic RecoveryInformation Provided by Teknor Apex |
|||
100% Modulus | 0.0145 GPa | 2.10 ksi | ASTM D412 |
Teknor Apex UNIPRENE® 7100-50D Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
100% Modulus | 0.0145 GPa | 2.10 ksi | ASTM D412 |
Lubrizol Estane® ETE 55DS3 Thermoplastic Polyurethane, Easy-to-Extrude Type: Estane® ETE 55DS3 is a 55D aromatic polyester-based thermoplastic polyurethane (TPU).Features: Hard TPU with wide extrusion processing window and melt stability, low temperature flexibility, .. |
|||
100% Modulus | 0.0145 GPa | 2.10 ksi | |
Elastomer Engineering E950-95A Polyurethane A general-purpose, high-tensile and high-load carrying polyether-based urethane.Information provided by Elastomer Engineering Inc (EEI) |
|||
100% Modulus | 0.0145 GPa | 2.10 ksi | ASTM D638 |
Colorite Polymers 9273E General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
100% Modulus | 0.0145 GPa | 2.10 ksi | ASTM D-638 |
Axiall 8916 Moldings & Extrusions Flexible PVC A satin finish extrusion compound best suited for extruded T-moldings, tubings and other shapes where uniform flow through the die is required. The compound exhibits excellent abrasion resistance.I.. |
|||
100% Modulus | 0.0145 GPa | 2.10 ksi | ASTM D-638 |
Axiall 8933 Moldings & Extrusions Flexible PVC General purpose extrusion compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.0145 GPa | 2.10 ksi | ASTM D-638 |
Axiall EX1063 Coax & Telecom Flexible PVC Non-lead stabilized, fiber optic compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.0145 GPa | 2.10 ksi | ASTM D-638 |
Axiall 4425 Flexible PVC Non-lead stabilized high speed TWP automotive insulation. Rated for a maximum service temperature of 85°C. Suitable for SAE J1128, SAE 1560, Ford MIL 120A and Chrysler MS 7889; MS-DC16 Type A.Inf.. |