Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.0130 GPa | 1.89 ksi | ISO 37 |
Huntsman AVALON® 95 AB Thermoplastic Polyurethane Introduction: AVALON 95 AB is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 95 AB is part of the AVALON Performance Range and offers a premium soling ma.. |
|||
100% Modulus | 0.0130 GPa | 1.89 ksi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-8195 Polyether-Based TPU Excellent hydrolytic stability, fungus resistance, low temperature flexibility & UV resistanceInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
100% Modulus | 0.0130 GPa | 1.89 ksi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-1495RV Polyester Based TPU Good extrusion stability, high transparency, excellent mechanical propertiesInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
100% Modulus | 0.0130 GPa | 1.89 ksi | ISO 37 |
ELASTO UK Dryflex® 9035-101 TPE, Modified Injection Molding Grade for Semi Rigid Molding The VTC TPE Group have developed endless formulations to fulfill different properties and application requirements to optimize the finished component. VTC Dryflex® 9035-101 is specifically designe.. |
|||
100% Modulus | 0.0130 GPa | 1.89 ksi | ASTM D412 |
C.O.I.M. LARIPUR® LPR5260 PTMG Polyether Polyurethane Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |
|||
100% Modulus | 0.0130 GPa | 1.88 ksi | ASTM D-638 |
Axiall 01560 Plenum Flexible PVC CAT 5 rated plenum jacket.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.0130 GPa | 1.89 ksi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-1595 Polyester Based TPU Low cost, good mechanical properties, good processabilityInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
100% Modulus | 0.0130 GPa | 1.89 ksi | ASTM D412-80 |
DuPont Performance Polymers Hypalon® 30 Chlorosulfonated Polyethylene Rubber, Carbon Black Filled Compound
(d Carbon black compound with 100 parts Hypalon; 27.8 parts sublimed litharge dispersion; 55 parts carbon black; 55 parts aromatic process oil; 0.5 parts MTBS; and 2 parts Tetrone® A rubber accelerato.. |
|||
100% Modulus | 0.0130 GPa | 1.89 ksi | Aged 1008 Hrs at 150°C in ASTM SF105 Oil |
DuPont Vamac® DHC Ethylene Acrylic Elastomer
(discontinued **) DuPont™ Vamac® DHC is a dipolymer of ethylene and methylacrylate cured using peroxide vulcanization systems. This gum elastomer includes a small amount of processing aid. It has a mild acrylic odo.. |
|||
100% Modulus | 0.0130 GPa | 1.89 ksi | ISO 37 |
Huntsman AVALON® 95 ABR Thermoplastic Polyurethane Introduction: AVALON 95 AB is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 95 AB is part of the AVALON Performance Range and offers a premium soling ma.. |