Polymer Property : 100% Modulus = 0.0118 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
100% Modulus 0.0118 GPa
1.71 ksi
ASTM D1414
Process Technologies Inc Sanifluor® 1000 Formulated Aflas® Elastomer
O-Rings, Gaskets and Seals produced from Sanifluor® 1000 have excellent chemical, heat and steam resistance. They provide superior performance in hot water, steam and virtually all caustics; makin..
100% Modulus 0.0118 GPa
1.71 ksi
Taiwan PU Corporation TPU-C95 General Grade, Calender Molding Polyester Base TPU
Thermoplastic Polyurethane (TPU), General Grade, Polyester Base, Calender MoldingInformation provided by Taiwan PU Corporation.
100% Modulus 0.0118 GPa
1.71 ksi
Taiwan PU Corporation TPU-CH95 High Hydrolysis Resistance, Calender Molding Polyether Base TPU
Thermoplastic Polyurethane (TPU), High Hydrolysis Resistance, Polyether Base, Calender MoldingInformation provided by Taiwan PU Corporation.
100% Modulus 0.0118 GPa
1.71 ksi
Taiwan PU Corporation TPU-E98 General Grade, Extrusion Molding Polyester Base TPU
Thermoplastic Polyurethane (TPU), General Grade, Polyester Base, Extrusion MoldingInformation provided by Taiwan PU Corporation.
100% Modulus 0.0118 GPa
1.71 ksi
Taiwan PU Corporation TPUI-T95 Transparent Grade, Injection Molding Polyester Base TPU
Thermoplastic Polyurethane (TPU), Transparent Grade, Polyester Base, Injection MoldingInformation provided by Taiwan PU Corporation.
100% Modulus 0.0118 GPa
1.71 ksi
500 mm/min; ASTM D 412
Zylog Neoplast® 240 FT EB Thermoplastic Vulcanizate
Neoplast 240 FT EB is a hard, dynamically vulcanized thermoplastic vulcanizate (TPV), based on polyolefin chemistry, and is intended for Injection Molding, Blow Molding and Extrusion applications.Ro..
100% Modulus 0.0118 GPa
1.71 ksi
DIN 53504
Lubrizol ESTANE® ETE50DT3 Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..