Mechanical Properties Metric English Comments
100% Modulus 0.0102 GPa
1.48 ksi
ASTM D412-80
DuPont Performance Polymers Hypalon® 48 Chlorosulfonated Polyethylene Rubber, Carbon Black Filled Compound  (d
Carbon black compound with 100 parts Hypalon; 27.8 parts sublimed litharge dispersion; 55 parts carbon black; 55 parts aromatic process oil; 0.5 parts MTBS; and 2 parts Tetrone® A rubber accelerato..
100% Modulus 0.0102 GPa
1.48 ksi
LG Chemical LGflex GL300 Plasticizer
Features: Excellent Viscosity, Heat Stability and Non-endocrine disrupterApplication: PVC Calenderings/Leathers, Sheets, Gloves, HoseInformation provided by LG Chemical
100% Modulus 0.0102 GPa
1.48 ksi
ASTM D412
Lubrizol Pellethane® 2363-90AE Thermoplastic Polyurethane Elastomer
Feature: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009.