Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00890 GPa | 1.29 ksi | DIN 53504 |
Huntsman IROGRAN® A 92 H 4656 Polyester-Based TPU-Injection Molding Grade Introduction: IROGRAN A 92 H 4656 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are short cycle times, good melt flow and e.. |
|||
100% Modulus | 0.00890 GPa | 1.29 ksi | DIN 53504 |
Lubrizol ESTANE® 5719 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |