Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : 100% Modulus = 0.00810 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
100% Modulus 0.00810 GPa
1.17 ksi
Press cure 10 Minutes @ 177°C, Post Cure 16 Hours @ 232°C
3M Dyneon™ 2299X Ultra High Viscosity Fluoroelastomer
3M™ Dyneon™ FC 2299X is an ultra high viscosity fluoroelastomers designed for use in applications such as o-rings, gaskets and seals requiring higher strength than achievable with lower viscosity ..
100% Modulus 0.00810 GPa
1.17 ksi
Press cure 10 Minutes @ 177°C, Post Cure 16 Hours @ 232°C
3M Dyneon™ 2299PX Ultra High Viscosity Fluoroelastomer
3M™ Dyneon™ FC 2299PX is an ultra high viscosity fluoroelastomers designed for use in applications such as o-rings, gaskets and seals requiring higher strength than achievable with lower viscosity..
Copyright © lookpolymers.com All Rights Reserved