Mechanical Properties Metric English Comments
100% Modulus 0.00800 GPa
1.16 ksi
ASTM D412
Precision Polymer Engineering Perlast® G60H Perfluoroelastomer
Special, pure white compound with excellent high temperature properties and wide chemical resistance. Extremely low outgassing properties.Applications: For use in applications which require exposur..
100% Modulus >= 0.00800 GPa
>= 1.16 ksi
DIN 53504
NEXA® PFX8014 Perfluoroelastomer
NEXA produces sealing elements for extreme and critical applications, particularly where high temperature, wet conditions (steam/water), purity and chemical resistance are important factors to consi..
100% Modulus >= 0.00800 GPa
>= 1.16 ksi
DIN 53504
NEXA® PFX8034 Perfluoroelastomer
NEXA produces sealing elements for extreme and critical applications, particularly where high temperature, wet conditions (steam/water), purity and chemical resistance are important factors to consi..
100% Modulus 0.00800 GPa
1.16 ksi
ASTM D412
Lubrizol Advanced Materials PEARLTHANE® D16N90UV Thermoplastic Polyurethane Elastomer  (discontinued **)
PEARLTHANE® D16N90UV is a polyether-based TPU, containing an anti-UV additive, supplied in form of transparent, colorless pellets, offering adequate hardness, excellent mechanical properties and go..
100% Modulus 0.00800 GPa
1.16 ksi
ISO 37
Huntsman AVALON® 90 AB Thermoplastic Polyurethane
Performance Features: AVALON® injection molding products are trusted worldwide to deliver:Outstanding flex performanceExcellent slip resistancePerfect surface definitionTransparency and transluce..
100% Modulus 0.00800 GPa
1.16 ksi
ASTM D412
Lubrizol Advanced Materials PEARLTHANE® 11T92EM Thermoplastic Polyurethane Elastomer
PEARLTHANE® 11T92EM is a polyester based TPU, supplied in form of translucent, colourless or slightly yellowish pellets, combining hardness with excellent mechanical properties. It can be extrude..
100% Modulus 0.00800 GPa
1.16 ksi
ISO 37
Huntsman AVALON® 90 ABR Thermoplastic Polyurethane
Introduction: AVALON 90 ABR is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 90 ABR is part of the AVALON Performance Range and offers a premium soling ..
100% Modulus 0.00800 GPa
1.16 ksi
ISO 37
Huntsman AVALON® 90 AK Thermoplastic Polyurethane
Introduction: AVALON 90 AK is a part of the AVALON Crystal Range and offers a specially designed, flexible material wit a higher degree of transparency compared with conventional TPU at the same har..
100% Modulus 0.00800 GPa
1.16 ksi
ISO 37
Huntsman AVALON® 90 AKU Thermoplastic Polyurethane
Introduction: AVALON 90 AKU is a part of the AVALON Crystal Range and offers a specially designed, flexible material wit a higher degree of transparency compared with conventional TPU at the same ha..
100% Modulus 0.00800 GPa
1.16 ksi
DIN 53504
Huntsman IROGRAN® A 92 E 4738 Polyester-Based TPU-Injection Extrusion Grade
Introduction: IROGRAN A 92 E 4738 is a white-colored, thermoplastic special-polyester-polyurethane for injection molding applications. Additional characteristics of the product are flexibility and h..
100% Modulus 0.00800 GPa
1.16 ksi
ASTM D412
Lubrizol STAT-RITE® S-1100 Static Dissipative TPU
Description: Stat-Rite® S1100 is a static dissipative TPU alloy. Stat-Rite S-1100 utilizes the patented Stat-Rite inherently dissipative polymer (IDP) alloy system to provide clean, permanent ESD p..
100% Modulus 0.00800 GPa
1.16 ksi
ASTM D412
Wanhua Chemical Wanthane® WHT-2190 Polycaprolactone Based TPU
Low compression set, good oil resistance & hydrolytic stability, good abrasion resistance, low temperature flexibilityInformation provided by Wanhua Chemical Group Co., Ltd.
100% Modulus 0.00800 GPa
1.16 ksi
ASTM D412
Wanhua Chemical Wanthane® WHT-7185 Polycaprolactone Based TPU
Higher mechanical strength, good hydrolytic stability & chemical resistance, weather resistance, heat & fungus resistanceInformation provided by Wanhua Chemical Group Co., Ltd.
100% Modulus 0.00800 GPa
1.16 ksi
DIN 53504
Lubrizol ESTANE® 58447 Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
100% Modulus 0.00800 GPa
1.16 ksi
ASTM D412
Wanhua Chemical Wanthane® WHT-1290 Polyester Based TPU
Good mechanical properties, good extrusion stability, low costInformation provided by Wanhua Chemical Group Co., Ltd.
100% Modulus 0.00800 GPa
1.16 ksi
ASTM D412
Wanhua Chemical Wanthane® WHT-1590 Polyester Based TPU
Low cost, good mechanical properties, good processabilityInformation provided by Wanhua Chemical Group Co., Ltd.
100% Modulus 0.00800 GPa
1.16 ksi
ASTM D412
Dow PELLETHANE® 2101-85A Polyurethane Elastomer (Ether-Ether Hybrid)  (discontinued **)
Description: PELLETHANE® 2101-85A offers good low temperature properties, fast cycle time, and good hydrolytic stability. Applications include: seals, gaskets, animal tags, molding applications, ho..