Polymer Property : 100% Modulus = 0.00550 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
100% Modulus 0.00550 GPa
0.798 ksi
DIN 53504
Huntsman IROGRAN® A 85 D 5001 Polyester-Based TPU-Injection Extrusion Grade
High Hydrolysis resistance and good crystallinity. Suggested for extrusion.Information provided by Huntsman
100% Modulus 0.00550 GPa
0.798 ksi
ISO 527-2/5A/500
Lubrizol Advanced Materials PEARLTHANE® 91T85 Thermoplastic Polyurethane Elastomer
Type : Pearlthane® 91T85 is a aliphatic-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Low density, fast processing and excellent elasticity properties.A..
100% Modulus 0.00550 GPa
0.797 ksi
Seals Eastern Perflas® 9291 Highly Fluorinated Fluoroelastomer Seals
Perflas 9291® seals are made of a chemical resistant highly fluorinated fluoroelastomer (FEPM - ASTM D1418 designated). Perflas9291 seals offer outstanding resistance to high temperatures (300Â..
100% Modulus 0.00550 GPa
0.798 ksi
Cecilia 20 aged 168 hrs at 175°C
DuPont Vamac® DP DIAK No. 7 Coagent Test Compound
Vamac® DP is an ethylene acrylic dipolymer elastomer. Its general performance characteristics are similar to those of the Vamac® terpolymers, including:Good oil and chemical resistanceHigh temper..
100% Modulus 0.00550 GPa
0.798 ksi
Lubrizol ESTANE® 5708 Ester Based Thermoplastic Polyurethane
Features: Very resilient product with excellent resistance to abrasion and tearing, low temperature flexibility, and resistant to certain chemicals.Uses: Hot melt adhesive, synthetic leather and fab..
100% Modulus 0.00550 GPa
0.797 ksi
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 1.0 PHR Thanecure® ZM
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
100% Modulus 0.00550 GPa
0.798 ksi
ASTM D412
Lubrizol Estane® 2102-80A Thermoplastic Polyurethane Elastomer
Formerly PellethaneFeature: Low compression setAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 20..
100% Modulus 0.00550 GPa
0.798 ksi
ASTM D412
Lubrizol Estane® 2103-80AE Thermoplastic Polyurethane Elastomer
Formerly PellethaneAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009.
100% Modulus 0.00550 GPa
0.798 ksi
ASTM D412
Lubrizol Estane® 2103-84AEN Thermoplastic Polyurethane Elastomer
Formerly PellethaneFeature: Contains UV Stabilizer, NSF Standard 61 certifiedAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pelletha..
100% Modulus 0.00550 GPa
0.798 ksi
Vulcanizate, Press cured, TC95 +3min at 160°C
Dow Nordel® IP 4725P General Purpose Molding
FormulationNordel® IP 4725P
100% Modulus 0.00550 GPa
0.798 ksi
ISO 37
AlphaGary Evoprene™ GC 5652 SEBS Thermoplastic Elastomer
Evoprene™ GC compounds are based on styrene ethylene- butylene styrene block copolymers. Evoprene™ GC series was created to provide cost effective solutions for processors and end users alike. Can..
100% Modulus 0.00550 GPa
0.797 ksi
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 1.0 PHR Thanecure® ZM
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
100% Modulus 0.00550 GPa
0.798 ksi
DIN 53504
Lubrizol ESTANE® 58202 Ether Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
100% Modulus 0.00550 GPa
0.798 ksi
ASTM D412
Lubrizol ESTANE® 58271 Ester Based Thermoplastic Polyurethane
Features: Good physical properties, chemical resistance and adhesive properties and wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection and blow molding.Avai..
100% Modulus 0.00550 GPa
0.798 ksi
ASTM D412
Lubrizol ESTANE® 58325 Ether Based Thermoplastic Polyurethane
Features: High melt strength for thick sheet extrusion.Uses: Blown and Flat Die/Cast Extrusion, Tubing and Profile ExtrusionAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformat..
100% Modulus 0.00550 GPa
0.798 ksi
ASTM D412
Lubrizol Estane® 58437 Thermoplastic Polyurethane
Type: Estane® 58437 is an 85A aromatic polyester-based thermoplastic polyurethane (TPU).Features: Excellent cold temperature properties and improved heat resistance.Uses: Blown and flat die/cast fi..
100% Modulus 0.00550 GPa
0.798 ksi
ASTM D412-80
DuPont Performance Polymers Hypalon® 40S Chlorosulfonated Polyethylene Rubber, Mineral Filled Compound  (disco
Mineral filled compound with 100 parts Hypalon; 80 parts hard clay; 4 parts magnesia; 30 parts aromatic process oil; 3 parts pentaerythritol; and 2 parts Tetrone® A rubber accelerator (from DuPont ..
100% Modulus 0.00550 GPa
0.798 ksi
ASTM D412
Lubrizol ESTANE® 58202 Ether Based Thermoplastic Polyurethane
Features: Halogenated flame retardant compound with good low temperature properties and cut resistanceUses: Extrusion – wire and cable jacketing and general extrusion where flame retardant properti..
100% Modulus 0.00550 GPa
0.798 ksi
ASTM D412
Lubrizol ESTANE® 58206 Ester Based Thermoplastic Polyurethane
Features: Good Flexibility at Low Temperatures and Improved Weathering Performance.Uses: Flat Die/Cast Film Extrusion and Hose/Profile Extrusion, Injection Molding.Available in Americas, Europe, Mid..