Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00440 GPa | 0.638 ksi | Injection molded parts; DIN 53504 |
Huntsman IROGRAN® A 78 E 4506 TPU-Polyester Introduction: IROGRAN A 78 E 4506 is a thermoplastic polyester- polyurethane for injection molding and extrusion applications. Additional characteristics of the product are excellent mechanical prop.. |
|||
100% Modulus | 0.00440 GPa | 0.638 ksi | |
Taiwan PU Corporation TPU-BTB85 Breathable Grade, Blow Molding Polyether Base TPU Thermoplastic Polyurethane (TPU), Breathable Grade, Polyether Base, Blow MoldingInformation provided by Taiwan PU Corporation. |
|||
100% Modulus | 0.00440 GPa | 0.638 ksi | |
Taiwan PU Corporation TPUI-L70 Low Temperature Resistance, Injection Molding Polyester Base TPU Thermoplastic Polyurethane (TPU), Low Temperature Resistance, Polyester Base, Injection MoldingInformation provided by Taiwan PU Corporation. |
|||
100% Modulus | 0.00440 GPa | 0.638 ksi | ASTM D412 |
UBE UBEPOL VCR412 Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C) Description: UBEPOL-VCR is a new type of synthetic rubber system developed by UBE's original technology. UBEPOL-VCR consists of micro-dispersed syndiotactic 1,2-polybutadiene (SPB) with high mel.. |
|||
100% Modulus | 0.00440 GPa | 0.638 ksi | ISO 37 |
Lubrizol ESTANE® 58280 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
100% Modulus | 0.00440 GPa @Temperature 23.0 °C |
0.638 ksi @Temperature 73.4 °F |
12 months, Weathering @ 45° South, 25 mil - Natural, Florida |
Lubrizol Estane® 58610 Thermoplastic Polyurethane Features: Combines flexibility, toughness and excellent roll release for calendering and melt coating applications.Uses: Injection molding and general extrusion techniques. It is used in film, shee.. |
|||
100% Modulus | 0.00440 GPa | 0.638 ksi | DIN 53504 |
Lubrizol ESTANE® 58561 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
100% Modulus | 0.00440 GPa | 0.638 ksi | ISO 37 |
ELASTO UK Dryflex® 8009-101 Flame Retardant TPE for Extrusion, Black Vitaprene® thermoplastic elastomers combine the performance of most vulcanized rubber with the process properties of thermoplastics. Vitaprene® compounds permit sophisticated component design and.. |
|||
100% Modulus | 0.00440 GPa | 0.638 ksi | ISO 37 |
ELASTO UK Dryflex® 8009-101 Flame Retardant TPE for Extrusion, Natural Vitaprene® thermoplastic elastomers combine the performance of most vulcanized rubber with the process properties of thermoplastics. Vitaprene® compounds permit sophisticated component design and.. |
|||
100% Modulus | 0.00440 GPa | 0.638 ksi | ISO 37 |
ELASTO UK Dryflex® 8009-101 Flame Retardant TPE for Injection Molding, Black Dryflex® thermoplastic elastomers combine the performance of most vulcanized rubber with the process properties of thermoplastics. Dryflex® compounds permit sophisticated component design and thu.. |
|||
100% Modulus | 0.00440 GPa | 0.638 ksi | ISO 37 |
ELASTO UK Dryflex® 8009-101 Flame Retardant TPE for Injection Molding, Natural Dryflex® thermoplastic elastomers combine the performance of most vulcanized rubber with the process properties of thermoplastics. Dryflex® compounds permit sophisticated component design and thu.. |
|||
100% Modulus | 0.00440 GPa | 0.638 ksi | Vulcanizate, Press cured, TC95 +3min at 160°C |
Dow Nordel® IP 4570 Dense Extruded Profile FormulationNordel® IP 4570 |
|||
100% Modulus | 0.00440 GPa | 0.638 ksi | Vulcanizate, Press cured, TC95 +3min at 160°C |
Dow Nordel® IP 5565 Dense Extruded Profile FormulationNordel® IP 5565 |
|||
100% Modulus | 0.00440 GPa | 0.638 ksi | ASTM D412 |
C.O.I.M. LARIPUR® LPR7560 PTMG Polyether Polyurethane Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |
|||
100% Modulus | 0.00440 GPa | 0.638 ksi | Cured 7 min at 177°C and Post Cured 2 hr at 232°C |
DuPont Performance Polymers VTR 8655 (GBL-S) , VTR 8650 8655/8650 Blend
(discontinued **) FormulationVTR 8655 |