Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00430 GPa | 0.624 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 60 PHR N774 (SRF) Filler MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00430 GPa | 0.624 ksi | DIN 53504 |
Huntsman IROGRAN® A 78 E 4588 Polyester-Based TPU-High Performance Grade High Hydrolysis resistance and good crystallinity. Suggested for injection molding.Information provided by Huntsman |
|||
100% Modulus | 0.00430 GPa | 0.624 ksi | DIN 53504 |
Lubrizol ESTANE® T5275 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
100% Modulus | 0.00430 GPa | 0.624 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 60 PHR N774 (SRF) Filler MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00430 GPa | 0.624 ksi | DIN 53504 |
Lubrizol ESTANE® T5192 Ether-Type Dissipative Compound (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
100% Modulus | 0.00430 GPa | 0.624 ksi | TPE-0153 (ASTM D 412) |
Advanced Elastomer Systems Santoprene® 251-85 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic flame retardant elastomer with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethylene. It can b.. |
|||
100% Modulus | 0.00430 GPa | 0.624 ksi | DIN 53504 |
Lubrizol ESTANE® 58245 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |