Polymer Property : 100% Modulus = 0.00360 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
100% Modulus 0.00360 GPa
0.522 ksi
TPE-0153 (ASTM D 412)
Advanced Elastomer Systems Santoprene® 281-73 Thermoplastic Rubber  (discontinued **)
A colorable thermoplastic medical grade elastomer with good fluid resistance, certified non-toxic by MEM elution test. It has USP Class VI Certificate of Compliance for biocompatibility and can be ..
100% Modulus 0.00360 GPa
0.522 ksi
TPE-0153 (ASTM D 412)
Advanced Elastomer Systems Trefsin® 3101-75 W305 Thermoplastic Rubber  (discontinued **)
A black thermoplastic elastomer with excellent permeation resistance to water, air and other gases. It can be processed using injection molding, extrusion, blow molding or other melt processing tec..
100% Modulus 0.00360 GPa
0.522 ksi
TPE-0153 (ASTM D 412)
Advanced Elastomer Systems Trefsin® 3201-75 W305 Thermoplastic Rubber  (discontinued **)
A natural thermoplastic elastomer with excellent permeation resistance to water, air and other gases. It can be processed using injection molding, extrusion, blow molding or other melt processing t..
100% Modulus 0.00360 GPa
0.522 ksi
DIN 53504
Huntsman IROGRAN® A 75 P 4665N TPU-Polyether
Excellent resistance to hydrolysis and microbial attack. Suggested for injection molding and extrusion.Information provided by Huntsman
100% Modulus 0.00360 GPa
0.522 ksi
Die C; Flow direction; ASTM D412
Teknor Apex Sarlink® 3170 Thermoplastic Elastomer
A medium hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3170 can be processed by blow molding, injection molding or..
100% Modulus 0.00360 GPa
0.522 ksi
Die C; Flow direction; ASTM D412
Teknor Apex Sarlink® 3470 Thermoplastic Elastomer
A NSF certified, medium hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inj..
100% Modulus 0.00360 GPa
0.522 ksi
Die C; Flow direction; ASTM D412
Teknor Apex Sarlink® 3470N Thermoplastic Elastomer
A NSF certified, colorable, multi-purpose thermoplastic elastomer featuring excellent fluid resistance and high temperature performance. It can be processed by injection molding, blow molding or ext..
100% Modulus 0.00360 GPa
0.522 ksi
ASTM D412
Teknor Apex Sarlink® 4380 Thermoplastic Elastomer
A highly engineered thermoplastic elastomer for use in demanding applications. Sarlink® 4380 is a flame retardant, medium hardness grade processing exceptional chemical resistance, compression s..
100% Modulus 0.00360 GPa
0.522 ksi
500 mm/min, measured parallel to flow; ISO 37
AlphaGary Evoprene™ LF 6154 Automotive Thermoplastic Elastomer
Evoprene™ LF is a hydrogenated styrene block copolymer based thermoplastic elastomer created for the automotive industry. It is specially formulated to have very low fogging characteristics suitab..
100% Modulus 0.00360 GPa
0.522 ksi
Press cure 10 Minutes @ 165°C, Ramp Post Cure in Air ASTM Die D Dumbbells
3M Dyneon™ 301Z Translucent Perfluoroelastomer System
Features and Benefits:Excellent plasma resistance with low particle count Low extractables, low outgassing, and low particle generation for ultra high purity applicationsPhosphorous-free and silica..
100% Modulus 0.00360 GPa
0.522 ksi
TPE-0153 (ASTM D 412)
Advanced Elastomer Systems Santoprene® 181-73 Thermoplastic Rubber  (discontinued **)
A black thermoplastic medical grade elastomer with good fluid resistance, certified non-toxic by MEM elution test. It has USP Class VI Certificate of Compliance for biocompatibility and can be proc..
100% Modulus 0.00360 GPa
0.522 ksi
Cured 7 min at 177°C and Post Cured 2 hr at 232°C
DuPont Performance Polymers VTR 8500 (GLT-S) 8500 Peroxide Cured Fluoroelastomer (FKM) Formulation  (discontin
FormulationViton® GLT