Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00340 GPa | 0.493 ksi | TPE-0153 (ASTM D 412) |
Advanced Elastomer Systems Santoprene® 221-73 W175 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic UV grade elastomer designed for thin wall extrusion applications with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and c.. |
|||
100% Modulus | 0.00340 GPa | 0.493 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 3.0 PHR Thanecure ZM MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00340 GPa | 0.493 ksi | DIN 53504 |
Huntsman IROGRAN® A 70 H 4673 M Polyester-Based TPU-Injection Molding Grade Introduction: IROGRAN A 70 H 4673 M is a soft polyester based thermoplastic polyurethane intended for injection molding applications. IROGRAN A 70 H 4673 M is part of the HUNTSMAN injection molding .. |
|||
100% Modulus | 0.00340 GPa | 0.493 ksi | 0.025" extruded film; DIN 53504 |
Huntsman IROGRAN® A 70 H 4714 M TPU-Polyester Introduction: IROGRAN A 70 H 4714 M is a soft polyester based thermoplastic polyurethane intended for injection molding applications. IROGRAN A 70 H 4714 M is part of the HUNTSMAN injection molding .. |
|||
100% Modulus | 0.00340 GPa | 0.493 ksi | |
Taiwan PU Corporation TPU-C75 General Grade, Calender Molding Polyester Base TPU Thermoplastic Polyurethane (TPU), General Grade, Polyester Base, Calender MoldingInformation provided by Taiwan PU Corporation. |
|||
100% Modulus | 0.00340 GPa | 0.493 ksi | |
Taiwan PU Corporation TPU-CH75 High Hydrolysis Resistance, Calender Molding Polyether Base TPU Thermoplastic Polyurethane (TPU), High Hydrolysis Resistance, Polyether Base, Calender MoldingInformation provided by Taiwan PU Corporation. |
|||
100% Modulus | 0.00340 GPa | 0.493 ksi | Die C; Cross direction; ASTM D412 |
Teknor Apex Sarlink® 4175 Thermoplastic Elastomer A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4175 is a medium hardness grade possessing exceptional tensile strength, superior compression set, chemical.. |
|||
100% Modulus | 0.00340 GPa | 0.493 ksi | Die C; Cross direction; ASTM D412 |
Teknor Apex Sarlink® 4475 Thermoplastic Elastomer A NSF certified, highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4475 is a medium hardness grade possessing exceptional tensile strength, superior compressio.. |
|||
100% Modulus | 0.00340 GPa | 0.493 ksi | ASTM D412 |
Lubrizol Estane® 58123 Thermoplastic Polyurethane Features: High moisture vapor transmission with low water swell and excellent low temperature and elasticity properties.Uses: Blown and flat die/cast film extrusion, injection molding and cable jack.. |
|||
100% Modulus | 0.00340 GPa | 0.493 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 3.0 PHR Thanecure ZM MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00340 GPa | 0.493 ksi | ASTM D412 |
Lubrizol Estane® MVT 70AT3 Thermoplastic Polyurethane, Moisture Vapor Transmission Type: Estane® MVT 70AT3 is an aromatic polyether-based thermoplastic polyurethane (TPU).Features: High moisture vapor transmission with low water swell. Excellent low temperature properties and el.. |
|||
100% Modulus | 0.00340 GPa | 0.493 ksi | ASTM D638 |
ELASTO UK Dryflex® 650800 TPE, Improved Compression Set and High Temperature Resistance, 80A Hardness The VTC TPE Group have developed endless formulations to fulfill different properties and application requirements to optimize the finished component. This grade is designed with improved compressi.. |
|||
100% Modulus | 0.00340 GPa | 0.493 ksi | Vulcanizate, Press cured, TC95 +3min at 160°C |
Dow Nordel® IP 4570 General Purpose Compound FormulationNordel® IP 4570 |
|||
100% Modulus | 0.00340 GPa | 0.493 ksi | DOWM 100789-LE90A |
Dow Tyrin® CM674 Elastomer Formulation FormulationTyrin® CPE Elastomer |
|||
100% Modulus | 0.00340 GPa | 0.493 ksi | TPE-0153 (ASTM D 412) |
ExxonMobil Vyram™ 9271-75 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic elastomer which complies with FDA regulations for rubber articles intended for repeated use, as well as rubber articles in contact with non-fatty, non-oily foods as closure.. |