Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00328 GPa | 0.475 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR N220 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00328 GPa | 0.475 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR N220 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00328 GPa | 0.475 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 45 PHR Mistron Vapor Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00328 GPa | 0.475 ksi | |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 0.5 PHR Sulfur MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
100% Modulus | 0.00328 GPa | 0.475 ksi | ASTM D-638 |
Axiall 8630 Moldings & Extrusions Flexible PVC Extrusion compound recommended for extruded shapes and other applications where a matte finish is desired.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.00328 GPa | 0.475 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 45 PHR Mistron Vapor Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00328 GPa | 0.475 ksi | |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 0.5 PHR Sulfur MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
100% Modulus | 0.00328 GPa | 0.475 ksi | ASTM D638 |
Colorite Polymers 5790 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |