Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00320 GPa | 0.464 ksi | TPE-0153 (ASTM D 412) |
Advanced Elastomer Systems Santoprene® 251-80 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic flame retardant elastomer with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethylene. It can b.. |
|||
100% Modulus | 0.00320 GPa | 0.464 ksi | ISO 37 |
Kuraray SEPTON® S2002 Thermoplastic Rubber SEPTON® is a series of high performance thermoplastic rubbers developed by Kuraray Co. Ltd. using its isoprene technology. SEPTON® resins are hydrogenated styrenic block copolymers, which exhi.. |
|||
100% Modulus | 0.00320 GPa | 0.464 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 6.0 PHR MBTS MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00320 GPa | 0.464 ksi | ASTM D412 |
C.O.I.M. LARIPUR® LPR7018 Plasticized Ester Polyurethane Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |
|||
100% Modulus | 0.00320 GPa | 0.464 ksi | ISO 37 |
AlphaGary Evoprene™ 049 Standard SBS Thermoplastic Elastomer Compound The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han.. |
|||
100% Modulus | 0.00320 GPa | 0.464 ksi | ISO 37 |
AlphaGary Evoprene™ Super G 934 SEBS Thermoplastic Elastomer Evoprene™ Super G compounds are high performance styrene ethylene- butylene styrene based thermoplastic elastomers. Evoprene™ Super G has improved heat resistance and improved recovery properties.. |
|||
100% Modulus | 0.00320 GPa | 0.464 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 6.0 PHR MBTS MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00320 GPa | 0.464 ksi | DIN 53504 |
Lubrizol ESTANE® 58213 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |