Mechanical Properties Metric English Comments
100% Modulus 0.00279 GPa
0.405 ksi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 60A, Black Peroxide Cure
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
100% Modulus 0.00279 GPa
0.405 ksi
ASTM D412
Elastocon TPE Technologies Elastocon® 8068N Thermoplastic Elastomer
Elastocon® 8068N is a colorable thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8068N is FDA compliant and well suited..
100% Modulus 0.00279 GPa
0.405 ksi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 3.0 PHR Di-Cup 40C Peroxide, Hardness 65A
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
100% Modulus 0.00279 GPa
0.405 ksi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 3.0 PHR Di-Cup 40C Peroxide, Hardness 65A
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
100% Modulus 0.00279 GPa
0.405 ksi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 60A, Black Peroxide Cure