Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00276 GPa | 0.400 ksi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, 400ºF Cure Temperature MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
100% Modulus | 0.00276 GPa | 0.400 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR Mistron Vapor Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00276 GPa | 0.400 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR N339 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00276 GPa | 0.400 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR N650 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00276 GPa | 0.400 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 75 PHR Iceberg Clay Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00276 GPa | 0.400 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 90 PHR N990 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00276 GPa | 0.400 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, Hardness 64A MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00276 GPa | 0.400 ksi | ASTM D412 |
Teknor Apex UNIPRENE® 7010-64 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
100% Modulus | 0.00276 GPa | 0.400 ksi | ASTM D412 |
Teknor Apex UNIPRENE® 7400-64 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
100% Modulus | 0.00276 GPa | 0.400 ksi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, 400ºF Cure Temperature MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
100% Modulus | 0.00276 GPa | 0.400 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, Hardness 64A MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00276 GPa | 0.400 ksi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, Hardness 83A MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
100% Modulus | 0.00276 GPa | 0.400 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR N339 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00276 GPa | 0.400 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR N650 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00276 GPa | 0.400 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 45 PHR N774 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00276 GPa | 0.400 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 75 PHR Iceberg Clay Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00276 GPa | 0.400 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 90 PHR N990 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00276 GPa | 0.400 ksi | ASTM D638 |
Colorite Polymers 92-623A General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
100% Modulus | 0.00276 GPa | 0.400 ksi | ASTM D638 |
Colorite Polymers MULTICHEM™ 6014 Vinyl-Urethane Blend Description: MULTICHEM™ is characterized by:Greater ResiliencyImproved ElasticityLow Temperature PropertiesLower ExtractabilityMolding and ExtrusionInformation provided by Colorite Polymers. |
|||
100% Modulus | 0.00276 GPa | 0.400 ksi | ASTM D-638 |
Axiall 8553 Moldings & Extrusions Flexible PVC A general purpose profile extrusion compound with excellent weathering properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.00276 GPa | 0.400 ksi | ASTM D412 |
Advanced Polymer Alloys DURACRYN 8060 NC/BK Thermoplastic Rubber Information provided by Advanced Polymer Alloys |
|||
100% Modulus | 0.00276 GPa | 0.400 ksi | ASTM D412; ISO 37 |
Advanced Polymer Alloys DuraGrip™ 6170 BK Melt Processable Elastomer DuraGrip™ 6170BK is designed to be a special purpose Melt Processable Elastomer (MPE) that is easy to use in injection molding and extrusion processes. DGR 6170BK has an excellent
soft touch feel a.. |
|||
100% Modulus | 0.00276 GPa | 0.400 ksi | ASTM D-638 |
Axiall 8542 Moldings & Extrusions Flexible PVC General purpose, flexible PVC compound recommended for extrusion or molding applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.00276 GPa | 0.400 ksi | After 7 days at 257°F (125°C); ASTM D573; ISO 188 |
Advanced Polymer Alloys Alcryn® 2060 BK Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |
|||
100% Modulus | 0.00276 GPa | 0.400 ksi | After 7 days at 257°F (125°C); ASTM D573; ISO 188 |
Advanced Polymer Alloys Alcryn® 2060 NC Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |
|||
100% Modulus | 0.00276 GPa | 0.400 ksi | After 7 days at 257°F (125°C); ASTM D573; ISO 188 |
Advanced Polymer Alloys Alcryn® 4660 BK Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |
|||
100% Modulus | 0.00276 GPa | 0.400 ksi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, Hardness 83A MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
100% Modulus | 0.00276 GPa | 0.400 ksi | ASTM D638 |
Colorite Polymers 6014 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
100% Modulus | 0.00276 GPa | 0.400 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 45 PHR N774 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00276 GPa | 0.400 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR Mistron Vapor Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |