Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00260 GPa | 0.377 ksi | ISO 37 |
Termopol Termoton® V2GA0065A TPV Compound Termoton®V, TPV compounds with a dynamically cured EPDM phase closely dispersed in a polyolefin phase (PP). Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable;.. |
|||
100% Modulus | 0.00260 GPa | 0.377 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 2.0 PHR Sulfur MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00260 GPa | 0.377 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 2.0 PHR Thanecure ZM MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00260 GPa | 0.377 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 40 PHR N774 (SRF) Filler MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00260 GPa | 0.377 ksi | ASTM D412 |
Teknor Apex Sarlink® 4370 Thermoplastic Elastomer A highly engineered thermoplastic elastomer for use in demanding applications. Sarlink® 4370 is a flame retardant, soft hardness grade exhibiting exceptional chemical resistance, compression set.. |
|||
100% Modulus | 0.00260 GPa | 0.377 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 0.50 PHR Zinc Stearate MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00260 GPa | 0.377 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 1.0 PHR MBT MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00260 GPa | 0.377 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 1.0 PHR Sulfur MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00260 GPa | 0.377 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 1.5 PHR Sulfur MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00260 GPa | 0.377 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 2.0 PHR Sulfur MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00260 GPa | 0.377 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 2.0 PHR Thanecure ZM MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00260 GPa | 0.377 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 40 PHR N774 (SRF) Filler MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00260 GPa | 0.377 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 0.25 PHR Zinc Stearate MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00260 GPa | 0.377 ksi | ISO 37 |
ELASTO UK Dryflex® 3031-102 TPE, Modified Injection Molding Grade for Auto Interior Parts The VTC TPE Group have developed endless formulations to fulfill different properties and application requirements to optimize the finished component. VTC Dryflex® 3031-102 is specifically designe.. |
|||
100% Modulus | 0.00260 GPa | 0.377 ksi | Vulcanizate, Press cured, TC95 +3min at 160°C |
Dow Nordel® IP 4520 General Purpose Molding FormulationNordel® IP 4520 |
|||
100% Modulus | 0.00260 GPa | 0.377 ksi | Vulcanizate, Press cured, TC95 +3min at 160°C |
Dow Nordel® IP 4640 Low Cost General Purpose Hose FormulationNordel® IP 4640 |
|||
100% Modulus | 0.00260 GPa | 0.377 ksi | ASTM D412 |
C.O.I.M. LARIPUR® LPR6515 Plasticized Ester Polyurethane Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |
|||
100% Modulus | 0.00260 GPa | 0.377 ksi | ASTM D412 |
C.O.I.M. LARIPUR® LPR6518 Plasticized Ester Polyurethane Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |
|||
100% Modulus | 0.00260 GPa | 0.377 ksi | ISO 37 |
AlphaGary Evoprene™ Super G 931 SEBS Thermoplastic Elastomer Evoprene™ Super G compounds are high performance styrene ethylene- butylene styrene based thermoplastic elastomers. Evoprene™ Super G has improved heat resistance and improved recovery properties.. |
|||
100% Modulus | 0.00260 GPa | 0.377 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 0.25 PHR Zinc Stearate MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00260 GPa | 0.377 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 1.0 PHR Sulfur MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00260 GPa | 0.377 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 1.5 PHR Sulfur MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00260 GPa | 0.377 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 0.50 PHR Zinc Stearate MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00260 GPa | 0.377 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 1.0 PHR MBT MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |