Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00224 GPa | 0.325 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 20 PHR Mistron Vapor Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00224 GPa | 0.325 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR N774 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00224 GPa | 0.325 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 45 PHR Suprex Clay Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00224 GPa | 0.325 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 60 PHR Hi-Sil 233 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00224 GPa | 0.325 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 60 PHR N990 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00224 GPa | 0.325 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, Hardness 75A MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00224 GPa | 0.325 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, Hardness 75A MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00224 GPa | 0.325 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 120 PHR Atomite Whiting Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00224 GPa | 0.325 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR N774 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00224 GPa | 0.325 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 45 PHR Suprex Clay Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00224 GPa | 0.325 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 60 PHR Hi-Sil 233 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00224 GPa | 0.325 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 120 PHR Atomite Whiting Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00224 GPa | 0.325 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 20 PHR Mistron Vapor Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00224 GPa | 0.325 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 60 PHR N990 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |