Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00220 GPa | 0.319 ksi | ISO/R527 |
Polykemi AB POLYelast TPE Z600 Thermoplastic Elastomer, SEBS-based Information provided by Polykemi AB |
|||
100% Modulus | 0.00220 GPa | 0.319 ksi | ISO/R527 |
Polykemi AB POLYelast TPE Z706EX Thermoplastic Elastomer, SEBS-based Information provided by Polykemi AB |
|||
100% Modulus | 0.00220 GPa | 0.319 ksi | TPE-0153 (ASTM D 412) |
ExxonMobil Vyram™ 9271-65 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic elastomer which complies with FDA regulations for rubber articles intended for repeated use, as well as rubber articles in contact with non-fatty, non-oily foods as closure.. |
|||
100% Modulus | 0.00220 GPa | 0.319 ksi | Formulation Example; Press Cure 7'/177ºC |
TSE Industries Millathane® 28 Millable Polyester Polyurethane Rubber Millathane 28 has excellent resistance to gas (e.g., nitrogen) permeability as well as very good abrasion resistance and low temperature properties. This polyurethane rubber was designed for automot.. |
|||
100% Modulus | 0.00220 GPa | 0.319 ksi | ISO 37 |
Kuraray SEPTON® S2004 Thermoplastic Rubber SEPTON® is a series of high performance thermoplastic rubbers developed by Kuraray Co. Ltd. using its isoprene technology. SEPTON® resins are hydrogenated styrenic block copolymers, which exhi.. |
|||
100% Modulus | 0.00220 GPa | 0.319 ksi | ISO 37 |
Kuraray SEPTON® S4033 Thermoplastic Rubber SEPTON® is a series of high performance thermoplastic rubbers developed by Kuraray Co. Ltd. using its isoprene technology. SEPTON® resins are hydrogenated styrenic block copolymers, which exhi.. |
|||
100% Modulus | 0.00220 GPa | 0.319 ksi | |
Kuraray SEPTON® S64 Soft Compound Description: SEPTON® is a series of high performance thermoplastic rubbers developed by Kuraray Co. Ltd. using its unique isoprene technology. SEPTON® resins are a series of hydrogenated styre.. |
|||
100% Modulus | 0.00220 GPa | 0.319 ksi | Die C; Flow direction; ASTM D412 |
Teknor Apex Sarlink® 3450 Thermoplastic Elastomer A NSF certified, low hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inject.. |
|||
100% Modulus | 0.00220 GPa | 0.319 ksi | ASTM D412 |
UBE UBEPOL BR100 Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C) Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Information provided by UBE. |
|||
100% Modulus | 0.00220 GPa | 0.319 ksi | ASTM D412 |
UBE UBEPOL BR150 Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C) Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Information provided by UBE. |
|||
100% Modulus | 0.00220 GPa | 0.319 ksi | ASTM D412 |
UBE UBEPOL BR340L Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C) Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Information provided by UBE. |
|||
100% Modulus | 0.00220 GPa | 0.319 ksi | ASTM D412 |
UBE UBEPOL VCR150 Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C) Description: UBEPOL-VCR is a new type of synthetic rubber system developed by UBE's original technology. UBEPOL-VCR consists of micro-dispersed syndiotactic 1,2-polybutadiene (SPB) with high mel.. |
|||
100% Modulus | 0.00220 GPa | 0.319 ksi | Formulation Example; Press Cure 7'/177ºC |
TSE Industries Millathane® 28 Millable Polyester Polyurethane Rubber Millathane 28 has excellent resistance to gas (e.g., nitrogen) permeability as well as very good abrasion resistance and low temperature properties. This polyurethane rubber was designed for automot.. |
|||
100% Modulus | 0.00220 GPa | 0.319 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 0.5 PHR Thanecure ZM MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00220 GPa | 0.319 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 2.0 PHR MBTS MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00220 GPa | 0.319 ksi | ASTM D412 |
UBE UBEPOL BR360L Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 35 Minutes at 145°C) Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Information provided by UBE. |
|||
100% Modulus | 0.00220 GPa | 0.319 ksi | ASTM D412 |
Elastocon TPE Technologies Elastocon® 8058N Thermoplastic Elastomer Elastocon® 8058N is a colorable thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8058N is FDA compliant and well suited.. |
|||
100% Modulus | 0.00220 GPa | 0.319 ksi | 20 in/min; ASTM D412 |
DuPont Performance Polymers Kalrez® 8475 FFKM Perfluoroelastomer Kalrez® Sahara™ 8475 has been specifically developed to meet the challenging requirements associated with sealing applications in semiconductor thermal processes (i.e., diffusion furnace, LPCVD, R.. |
|||
100% Modulus | 0.00220 GPa | 0.319 ksi | ASTM D412 |
Elastocon TPE Technologies Elastocon® CLR65 Thermoplastic Elastomer Elastocon® CLR65 is a transparent thermoplastic elastomer that has been developed for applications that require oil/plasticizer free, high strength properties and a tactile surface finish. Elastoc.. |
|||
100% Modulus | 0.00220 GPa | 0.319 ksi | ISO 37 |
AlphaGary Evoprene™ 036 Standard SBS Thermoplastic Elastomer Compound The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han.. |
|||
100% Modulus | 0.00220 GPa | 0.319 ksi | ASTM D412 |
Advanced Polymer Alloys DuraGrip™ DGR 6160 NC Thermoplastic Elastomer (TPE) DuraGrip® DGR 6160 is offered in an NC (colorable) version, and is designed to chemically bond to a wide variety of thermoplastic substrates including ABS, PC, Nylon 6,
Nylon 6/6, glass filled Nylo.. |
|||
100% Modulus | 0.00220 GPa | 0.319 ksi | ASTM D 638 |
API Megol AM T A SEBS Adhesion Modified Overmolding for Polar Polymers Over-molding allows for the creation of composite finished products in a single phase, removing the need for successive gluing or mechanical fixing steps. This also reduces environmental impact as .. |
|||
100% Modulus | 0.00220 GPa | 0.319 ksi | ISO 37 |
AlphaGary Evoprene™ CE 6186 Thermoplastic Elastomer The Evoprene™ CE range has been specially created to offer processors a cost engineered range of easy processing, fast cycling thermoplastic elastomer compounds for general purpose applications. E.. |
|||
100% Modulus | 0.00220 GPa | 0.319 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 0.5 PHR Thanecure ZM MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00220 GPa | 0.319 ksi | Die C; Flow direction; ASTM D412 |
Teknor Apex Sarlink® 3150 Thermoplastic Elastomer A low hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3150 can be processed by injection molding or extrusion for appl.. |
|||
100% Modulus | 0.00220 GPa | 0.319 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 2.0 PHR MBTS MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00220 GPa | 0.319 ksi | ASTM D412 |
Elastocon TPE Technologies Elastocon® OF65 Thermoplastic Elastomer Elastocon® OF65 is a natural thermoplastic elastomer that has been developed for applications that require oil/plasticizer free, non-blooming high strength properties and a reduced coefficient of f.. |