Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00167 GPa | 0.242 ksi | |
Shin-Etsu Silicones LIMSâ„¢ KE1950-50A/B Elastomer KE-1950-50 is a liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. It's viscosity is low enough to allow easy .. |
|||
100% Modulus | 0.00167 GPa | 0.242 ksi | ASTM D412; ISO 37 |
Advanced Polymer Alloys DuraGrip™ DGR 6070 NC Thermoplastic Elastomer (TPE) DuraGrip® DGR 6070NC is designed to be a general purpose Thermoplastic Elastomer (TPE) that is easy to use in injection molding and extrusion processes. DGR 6070NC has an
excellent soft touch feel,.. |