Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hydrostatic Design Basis | 8.62 MPa @Temperature 23.0 °C |
1250 psi @Temperature 73.4 °F |
ASTM D 2837 |
Total Finathene® 3802N Natural HDPE pipe grade
(discontinued **) Applications: Natural gas distribution, extruded pipes, molded fittings, pipe coating, pipe liningInformation provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and .. |
|||
Hydrostatic Design Basis | 8.62 MPa | 1250 psi | @ 23 C; ASTM D2837 |
Ineos K38-20-160 Polyethylene Copolymer K38-20-160 is a medium density polyethylene copolymer containing an organic yellow pigment system, designed specifically for the extrusion of natural gas pipe. It exhibits excellent long term stres.. |
|||
Hydrostatic Design Basis | 8.618 MPa | 1250 psi | @23c; ASTM D 2837 |
Ineos K38-20X2091 HDPE K38-20X2091 is a yellow medium density polyethylene resin designed specifically for natural gas pipe extrusion. It exhibits excellent long term stress life and slow crack growth resistance. This m.. |