Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 108 J @Thickness 3.17 mm, Temperature -40.0 °C |
79.7 ft-lb @Thickness 0.125 in, Temperature -40.0 °F |
Rotational Molded, Instrumented |
NOVA Chemicals Surpass® RMs539-U Octene sMDPE Rotational Molding Film Features: Octene copolymerExceptional low temperature impact propertiesOutstanding stiffnessBroad processing windowSuperior whiteness for improved part appearanceEasy mold releaseNSF listed for Stan.. |
|||
Impact Test | 108 J @Thickness 3.17 mm, Temperature -40.0 °C |
79.7 ft-lb @Thickness 0.125 in, Temperature -40.0 °F |
Rotational Molded, Instrumented |
NOVA Chemicals Surpass® RMs539-UG Octene sMDPE Rotational Molding Film Features: Octene copolymerExceptional low temperature impact propertiesOutstanding stiffnessBroad processing windowSuperior whiteness for improved part appearanceEasy mold releaseNSF listed for Stan.. |